Defect studies of zirconia implanted by high energy Xe ions

The result's identifiers

  • Result code in IS VaVaI

    <a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216208%3A11320%2F16%3A10330793" target="_blank" >RIV/00216208:11320/16:10330793 - isvavai.cz</a>

  • Result on the web

    <a href="http://dx.doi.org/10.1088/1742-6596/674/1/012016" target="_blank" >http://dx.doi.org/10.1088/1742-6596/674/1/012016</a>

  • DOI - Digital Object Identifier

    <a href="http://dx.doi.org/10.1088/1742-6596/674/1/012016" target="_blank" >10.1088/1742-6596/674/1/012016</a>

Alternative languages

  • Result language

    angličtina

  • Original language name

    Defect studies of zirconia implanted by high energy Xe ions

  • Original language description

    In the present work positron lifetime spectroscopy was employed for characterization of radiation-induced defects in yttria stabilized zirconia (YSZ) implanted by 167 MeV Xe ions. Positron lifetime data were interpreted with aid of ab-initio theoretical modelling of defects in YSZ lattice. Damage caused by Xe implantation was investigated in two YSZ samples with different microstructure: (i) single crystal and (ii) sintered ceramic. The virgin YSZ single crystal exhibits single component spectrum with lifetime of approximate to 180 ps. Similar lifetime component was found also in the virgin sample of sintered YSZ ceramic. Since this lifetime is significantly higher than the YSZ bulk lifetime the virgin YSZ crystal and the sintered ceramic both contain vacancy-like defects. Xe implantation leads to appearance of additional defect component with longer lifetime approximate to 370 ps which comes obviously from vacancy clusters formed by agglomeration of irradiation induced vacancies. A broad absorption band with peak absorption at approximate to 518 nm was found in Xe-implanted crystal by optical measurements.

  • Czech name

  • Czech description

Classification

  • Type

    D - Article in proceedings

  • CEP classification

    JH - Ceramics, fire-proof materials and glass

  • OECD FORD branch

Result continuities

  • Project

    <a href="/en/project/GAP108%2F11%2F1396" target="_blank" >GAP108/11/1396: Effect of substitutional elements and grain boundaries on properties of nanocrystalline zirconia-based materials</a><br>

  • Continuities

    P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)

Others

  • Publication year

    2016

  • Confidentiality

    S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů

Data specific for result type

  • Article name in the collection

    Journal of Physics: Conference Series

  • ISBN

  • ISSN

    1742-6588

  • e-ISSN

  • Number of pages

    8

  • Pages from-to

  • Publisher name

    IOP PUBLISHING LTD

  • Place of publication

    BRISTOL

  • Event location

    Kyoto

  • Event date

    Sep 14, 2014

  • Type of event by nationality

    WRD - Celosvětová akce

  • UT code for WoS article

    000382077100016