Friction stir processing of hybridized AZ31B magnesium alloy-based composites by adding CeO2 and ZrO2powders: mechanical, wear, and corrosion behaviors
The result's identifiers
Result code in IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216208%3A11320%2F23%3A10474212" target="_blank" >RIV/00216208:11320/23:10474212 - isvavai.cz</a>
Result on the web
<a href="https://verso.is.cuni.cz/pub/verso.fpl?fname=obd_publikace_handle&handle=TzJOSNAKEE" target="_blank" >https://verso.is.cuni.cz/pub/verso.fpl?fname=obd_publikace_handle&handle=TzJOSNAKEE</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.jmrt.2023.03.028" target="_blank" >10.1016/j.jmrt.2023.03.028</a>
Alternative languages
Result language
angličtina
Original language name
Friction stir processing of hybridized AZ31B magnesium alloy-based composites by adding CeO2 and ZrO2powders: mechanical, wear, and corrosion behaviors
Original language description
To improve the properties of AZ31B Mg alloy and for the first time, the rare earth cerium oxide (CeO2) and zirconium dioxide (ZrO2) were combined for synergistic benefits and introduced into the structural AZ31B magnesium alloy through the solid-state friction stir processing procedure to form the hybridized AZ31B Mg/ZrO2+CeO2 composites under variable levels of the tool's rotational speed up to 1200 rpm. The macro-/microstructure, hardness, shear punching strength, tensile strength, corrosion behaviours, and tribological characteristics such as weight/wear loss, wear rate, coefficient of friction, worn surfaces, and debris of the AZ31B Mg/ZrO2+CeO2 hybrid composites were investigated and compared. The results indicated that void, tunnel defect, and ZrO2+CeO2 agglomeration could not be prevented at low speed (800 rpm) while defect-free composites were obtained at high speed (1200 rpm). Grain refinement from 7.39 mm to 3.38 mm and the ZrO2+CeO2 fragmentation (4.52-2.49 mm) ensued after a rise in the tool's rotational speed owing to higher plastic straining, dynamic recrystallization, and ZrO2+CeO2 particle-aided pinning effects. Improvements in hardness (99-135 HV), shear punching strength (121-237 MPa), tensile strength (172-228 MPa) and wear properties of the composite were attained due to the defect elimination, inherent finer Mg grains, and the uniformly dispersed ZrO2+CeO2 particles. These attributes also enhanced the corrosion resistance of the AZ31B Mg/ ZrO2+CeO2 composite at the elevated rotating speed of the tool. The combination of the CeO2 and ZrO2 particles is an effective particle-blend for improving the properties of Mg alloy to expand its application scope.(c) 2023 The Author(s). Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
Czech name
—
Czech description
—
Classification
Type
J<sub>imp</sub> - Article in a specialist periodical, which is included in the Web of Science database
CEP classification
—
OECD FORD branch
10302 - Condensed matter physics (including formerly solid state physics, supercond.)
Result continuities
Project
—
Continuities
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Others
Publication year
2023
Confidentiality
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Data specific for result type
Name of the periodical
Journal of Materials Research and Technology
ISSN
2238-7854
e-ISSN
2214-0697
Volume of the periodical
24
Issue of the periodical within the volume
3
Country of publishing house
BR - BRAZIL
Number of pages
24
Pages from-to
1949-1972
UT code for WoS article
000964628000001
EID of the result in the Scopus database
2-s2.0-85151258304