Influence of long-term ageing upon the capacity of hydrogen storage in two novel Mg-Ni-In-C alloys

The result's identifiers

  • Result code in IS VaVaI

    <a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26620%2F16%3APU143715" target="_blank" >RIV/00216305:26620/16:PU143715 - isvavai.cz</a>

  • Result on the web

    <a href="http://www.kovmat.sav.sk/article.php?rr=54&cc=6&ss=389" target="_blank" >http://www.kovmat.sav.sk/article.php?rr=54&cc=6&ss=389</a>

  • DOI - Digital Object Identifier

    <a href="http://dx.doi.org/10.4149/km_2016_6_389" target="_blank" >10.4149/km_2016_6_389</a>

Alternative languages

  • Result language

    angličtina

  • Original language name

    Influence of long-term ageing upon the capacity of hydrogen storage in two novel Mg-Ni-In-C alloys

  • Original language description

    We have shown previously that the addition of In and C enhances the hydrogen desorption capacity and considerably improves the kinetics of hydrogen desorption from Mg-Ni based alloys, important from the perspective of hydrogen storage. In this paper, we present the results of tests of the long-term stability of the sorption behaviour of these materials. We studied how the capacity and sorption kinetics changed 5 years from the preparation of two chosen Mg-Ni-In-C alloys differing in indium concentration. Kinetic curves and PCT isotherms were measured at temperatures of 250-350 degrees C. It was found that long-term storage of the hydrogen charged samples led to no significant downgrade in hydrogen sorption kinetics. However, the absorption capacity somewhat decreased from about 5 wt.% H-2 to about 3 wt.% H-2 due to partial phase decomposition. Relatively intensive tentative oxidation during preparation, which had a slightly beneficial effect on the desorption rate of freshly-prepared samples, caused almost total blocking of hydrogen sorption in the aged samples.

  • Czech name

  • Czech description

Classification

  • Type

    J<sub>imp</sub> - Article in a specialist periodical, which is included in the Web of Science database

  • CEP classification

  • OECD FORD branch

    20506 - Coating and films

Result continuities

  • Project

    <a href="/en/project/ED1.1.00%2F02.0068" target="_blank" >ED1.1.00/02.0068: Central european institute of technology</a><br>

  • Continuities

    P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)

Others

  • Publication year

    2016

  • Confidentiality

    S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů

Data specific for result type

  • Name of the periodical

    KOVOVE MATERIALY-METALLIC MATERIALS

  • ISSN

    0023-432X

  • e-ISSN

    1338-4252

  • Volume of the periodical

    54

  • Issue of the periodical within the volume

    6

  • Country of publishing house

    SK - SLOVAKIA

  • Number of pages

    8

  • Pages from-to

    389-396