Grain refinement of AZ61 alloy after ECAP processing

The result's identifiers

  • Result code in IS VaVaI

    <a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27360%2F17%3A10229656" target="_blank" >RIV/61989100:27360/17:10229656 - isvavai.cz</a>

  • Alternative codes found

    RIV/61989100:27230/17:10229656

  • Result on the web

    <a href="https://www.scientific.net/MSF.891.372" target="_blank" >https://www.scientific.net/MSF.891.372</a>

  • DOI - Digital Object Identifier

    <a href="http://dx.doi.org/10.4028/www.scientific.net/MSF.891.372" target="_blank" >10.4028/www.scientific.net/MSF.891.372</a>

Alternative languages

  • Result language

    angličtina

  • Original language name

    Grain refinement of AZ61 alloy after ECAP processing

  • Original language description

    Electron microscopy techniques were used to characterize the microstructure and deformation behavior of AZ61 alloy proceeded by ECAP. The commercial AZ61 alloy subjected to severe plastic deformation possesses a two-phase microstructure consisting of solid solution matrix and massive γ-phase Mg17Al12, or Mg17(Al,Zn)12 distributed mostly at grain boundaries. Based on selected area diffraction and electron back scattered diffraction applied to a sample after the third pass, it can be concluded that plastic deformation induced by ECAP occurs mainly by slip mode forming a high density network of dislocation inside the grains. The grains size was significantly refined to 1.4 µm after the third pass of ECAP. The refinement of grain size is probably due to polygonization process associated with formation of high angle grain boundaries due to dislocations rearrangement. Mg17(Al, Zn)12 precipitates of size scattered from 100 to 200 nm and also the primary precipitates of Al6Mn phase were observed in this alloy.

  • Czech name

  • Czech description

Classification

  • Type

    J<sub>SC</sub> - Article in a specialist periodical, which is included in the SCOPUS database

  • CEP classification

  • OECD FORD branch

    20301 - Mechanical engineering

Result continuities

  • Project

    <a href="/en/project/EE2.3.20.0038" target="_blank" >EE2.3.20.0038: Creation of an international team of scientists and participation in scientific networks in the sphere of nanotechnology and unconventional forming material</a><br>

  • Continuities

    P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)

Others

  • Publication year

    2017

  • Confidentiality

    S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů

Data specific for result type

  • Name of the periodical

    Materials science forum. Volume 891

  • ISSN

    0255-5476

  • e-ISSN

  • Volume of the periodical

    891

  • Issue of the periodical within the volume

    1

  • Country of publishing house

    CH - SWITZERLAND

  • Number of pages

    5

  • Pages from-to

    372-376

  • UT code for WoS article

  • EID of the result in the Scopus database

    2-s2.0-85016978197