Hydration and rheology of activated ultra-fine ground granulated blast furnace slag with carbide slag and anhydrous phosphogypsum
The result's identifiers
Result code in IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27690%2F22%3A10250470" target="_blank" >RIV/61989100:27690/22:10250470 - isvavai.cz</a>
Result on the web
<a href="https://www.sciencedirect.com/science/article/pii/S0958946522003201" target="_blank" >https://www.sciencedirect.com/science/article/pii/S0958946522003201</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.cemconcomp.2022.104727" target="_blank" >10.1016/j.cemconcomp.2022.104727</a>
Alternative languages
Result language
angličtina
Original language name
Hydration and rheology of activated ultra-fine ground granulated blast furnace slag with carbide slag and anhydrous phosphogypsum
Original language description
In this study, two different ultra-fine ground granulated blast furnace slag referred to as GS (i.e., by dry -winnowing method) and WS (i.e., by wet-grinding method) were obtained, and the hydration and rheology of activated ultra-fine ground granulated blast furnace slag (activated-BFS) with carbide slag and anhydrous phosphogypsum (AG) as combined activator were systematically investigated by means of setting time, work-ability, rheological behavior, compressive strength, autogenous shrinkage, electrical resistivity, SEM, XRD and TG-DTG. The results showed that the limiting factor is the BFS type, and not the AG dosage in terms of setting time, and their rheological behavior fitted with H-B model. WS and increase in AG dosage significantly reduced the plastic viscosity, shear stress and yield stress of activated-BFS pastes. The WS presented higher initial reaction activity that generated more hydrates in the early age, restricting the further hydration of BFS particles especially when AG dosage exceeded 10%, thus leading to the different compressive strength development trends between mixtures containing WS (WS/A) and GS (GS/A). The compressive strength of GS/A mixtures increased with increasing AG dosage and reached 39.9 MPa at 3 days, while WS/A first increased and then decreased. The activated-BFS with carbide slag and AG is technically feasible to be employed as cementitious materials in the production of concrete.
Czech name
—
Czech description
—
Classification
Type
J<sub>imp</sub> - Article in a specialist periodical, which is included in the Web of Science database
CEP classification
—
OECD FORD branch
20500 - Materials engineering
Result continuities
Project
—
Continuities
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Others
Publication year
2022
Confidentiality
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Data specific for result type
Name of the periodical
Cement and Concrete Composites
ISSN
0958-9465
e-ISSN
1873-393X
Volume of the periodical
133
Issue of the periodical within the volume
133
Country of publishing house
US - UNITED STATES
Number of pages
12
Pages from-to
nestrankovano
UT code for WoS article
000855169400001
EID of the result in the Scopus database
—