Mechanical properties of concrete with Recycled Aggregate
The result's identifiers
Result code in IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68407700%3A21110%2F14%3A00218932" target="_blank" >RIV/68407700:21110/14:00218932 - isvavai.cz</a>
Result on the web
—
DOI - Digital Object Identifier
—
Alternative languages
Result language
čeština
Original language name
Mechanické vlastnosti betonu s recyklovaným kamenivem
Original language description
This article deals with mechanical properties of concrete containing recycled concrete aggregate. Two types of recycled concrete aggregate were used for the production of the concrete, which originate from the same recycling center. First, the physical properties of the recycled aggregate were tested. Pycnometric test was used to test absorption and bulk density of the recycled aggregate. Previous research showed that these are properties with the greatest difference between natural and recycled aggregates. The test results were compared with the natural aggregates. The measurements showed that water absorption of the recycled aggregate is about seven times higher in larger fraction and ten times larger compared to natural aggregate. Decrease of weightwas about 18 %. For the testing of concrete, a total of six compounds were made, one of which was a reference compound and in others a coarse fraction of natural aggregate was in varying ratio replaced by recycled aggregate. The test res
Czech name
Mechanické vlastnosti betonu s recyklovaným kamenivem
Czech description
This article deals with mechanical properties of concrete containing recycled concrete aggregate. Two types of recycled concrete aggregate were used for the production of the concrete, which originate from the same recycling center. First, the physical properties of the recycled aggregate were tested. Pycnometric test was used to test absorption and bulk density of the recycled aggregate. Previous research showed that these are properties with the greatest difference between natural and recycled aggregates. The test results were compared with the natural aggregates. The measurements showed that water absorption of the recycled aggregate is about seven times higher in larger fraction and ten times larger compared to natural aggregate. Decrease of weightwas about 18 %. For the testing of concrete, a total of six compounds were made, one of which was a reference compound and in others a coarse fraction of natural aggregate was in varying ratio replaced by recycled aggregate. The test res
Classification
Type
D - Article in proceedings
CEP classification
JN - Civil engineering
OECD FORD branch
—
Result continuities
Project
—
Continuities
S - Specificky vyzkum na vysokych skolach
Others
Publication year
2014
Confidentiality
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Data specific for result type
Article name in the collection
Juniorstav 16.odborná konference doktorského studia
ISBN
978-80-214-4851-3
ISSN
—
e-ISSN
—
Number of pages
6
Pages from-to
—
Publisher name
Vysoké učení technické v Brně, Fakulta stavební
Place of publication
Brno
Event location
Brno
Event date
Jan 30, 2014
Type of event by nationality
EUR - Evropská akce
UT code for WoS article
—