Original language description
The paper shows the evaluation of delamination of HDG coating. The HDG coating adhesion was evaluated by impact test and by pull-off test. The effect of substrate steel chemical composition, metallurgical conditions and other parameters influencing the quality of zinc coating, mainly the intermetallic phases, are described. The silicon content in aluminium-killed steel was identified as crucial factor for tested samples. The result of adhesion test corresponds to structure of zinc coating.
Czech name
—
Czech description
—
Classification
Type
D - Article in proceedings
CEP classification
JK - Corrosion and material surfaces
OECD FORD branch
—
Result continuities
Project
—
Continuities
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Others
Publication year
2016
Confidentiality
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Data specific for result type
Article name in the collection
Metal 2016: 25th International Conference on Metallurgy and Materials
ISBN
978-80-87294-67-3
ISSN
—
e-ISSN
—
Number of pages
6
Pages from-to
904-909
Publisher name
Tanger
Place of publication
Ostrava
Event location
Brno
Event date
May 25, 2016
Type of event by nationality
WRD - Celosvětová akce
UT code for WoS article
000391251200146