Result

Quantitative Fractography of Fatigue Long Crack Growth under Remote Shear Loading Modes

Quantitative Fractography of Fatigue Long Crack Growth under Remote Shear Loading Modes...

JL - Únava materiálu a lomová mechanika

  • 2008
  • D
Result

Computer aided fractography: methods for evaluation of image anisotropy

Computer aided fractography: methods for evaluation of image anisotropy...

BA - Obecná matematika

  • 1999
  • D
Result

Application of 3D surface topography in fractography

Contribution describes ability of Talysurf CLI 1000 apparatus for analysis of surface topography and its applications in fractography. Advantages of 3D surface topography, limitations and examples are mentioned, too....

JL - Únava materiálu a lomová mechanika

  • 2006
  • D
Result

Analysis of microstucture and fracture surface of forged crankshafts

Evaluation of causes of failure included fractography analysis as well as investigation microstructure of material...

Materials engineering

  • 2017
  • Vsouhrn
Result

Contribution to the quantitative fractography of bainitic high-strength steel using the fractal analysis

Contribution to the quantitative fractography of bainitic high-strength steel using the fractal analysis...

JG - Hutnictví, kovové materiály

  • 1999
  • D
Result

Fractography of MCC produced by diffusion of Ni into Al

In-situ composites produced by diffusion of Ni plasma-sprayed coatings into the Al substrates and their properties.

JG - Hutnictví, kovové materiály

  • 2001
  • Jx
Result

Fracture analysis of coiled springs

Evalution of the failure causes by fractography analysis and complex evaluation of material, its mechanical properties and microstructure.

Materials engineering

  • 2017
  • Vsouhrn
Result

Failure investigation of threaded brass inserts

Objective of the analysis was to find the causes of failure by material investigation of fractured and nonfractured brass inserts along with fractography analysis......

Materials engineering

  • 2017
  • Vsouhrn
Result

Fractography Benefit to the Evaluation of Service Life of Power Plants Structural Components

, A508, 10GN2MFA, etc.). The importance and irreplaceable role of fractography of fractography is exampled by a case study dealing with the service failure of turbine blades....

JF - Jaderná energetika

  • 2008
  • D
Result

Analysis pin

Analysis pin - metallographic test, Microstructure of steel, hardness test HV, microhardness measurements, detailed analysis of the refractive Fractography, Electron microanalysis....

JJ - Ostatní materiály

  • 2012
  • O