Alkali-activated Slag Mortar Containing Alternative Activator: Long-Term Mechanical Fracture Parameters

The result's identifiers

  • Result code in IS VaVaI

    <a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26110%2F20%3APU138564" target="_blank" >RIV/00216305:26110/20:PU138564 - isvavai.cz</a>

  • Result on the web

    <a href="http://tces.vsb.cz/Home/ArticleDetail/506" target="_blank" >http://tces.vsb.cz/Home/ArticleDetail/506</a>

  • DOI - Digital Object Identifier

    <a href="http://dx.doi.org/10.35181/tces-2020-0014" target="_blank" >10.35181/tces-2020-0014</a>

Alternative languages

  • Result language

    angličtina

  • Original language name

    Alkali-activated Slag Mortar Containing Alternative Activator: Long-Term Mechanical Fracture Parameters

  • Original language description

    This paper deals with the determination of long-term mechanical fracture properties of alkali-activated slag (AAS) mortars with the alternative activator. Waste sludge from the production of waterglass was used as a sole alkaline activator for ground granulated blast furnace slag. Two types of sand were used to prepare two different mortar sets: standardized siliceous CEN sand consisting of three fractions according to EN 196-1 and natural sand with a nominal grain size up to 4 mm. The results of the elastic, fracture and strength parameters for both sets of AAS mortars determined within the time interval of 3 to 650 days of ageing are summarized in the paper. The obtained results show a different trend in the development of the material properties of AAS mortars compared to the ordinary cement-based mortars which should be taken into the account in the material specification for practical application. It seems that the hardening process influencing the mechanical fracture characteristics is more progressive after the age of 28 days.

  • Czech name

  • Czech description

Classification

  • Type

    J<sub>ost</sub> - Miscellaneous article in a specialist periodical

  • CEP classification

  • OECD FORD branch

    20101 - Civil engineering

Result continuities

  • Project

    <a href="/en/project/GJ18-12289Y" target="_blank" >GJ18-12289Y: Advanced characterization of cracks propagation in composites based on alkali activated matrix</a><br>

  • Continuities

    P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)

Others

  • Publication year

    2020

  • Confidentiality

    S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů

Data specific for result type

  • Name of the periodical

    Sborník vědeckých prací Vysoké školy báňské – Technické univerzity Ostrava

  • ISSN

    1213-1962

  • e-ISSN

  • Volume of the periodical

    2020

  • Issue of the periodical within the volume

    2

  • Country of publishing house

    CZ - CZECH REPUBLIC

  • Number of pages

    8

  • Pages from-to

    28-35