Biodegradable Zn-0.8Mg-0.2Sr alloy as an internal fixation material exhibits controlled degradation with enhanced osteogenesis

The result's identifiers

  • Result code in IS VaVaI

    <a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68378271%3A_____%2F25%3A00638536" target="_blank" >RIV/68378271:_____/25:00638536 - isvavai.cz</a>

  • Alternative codes found

    RIV/60461373:22310/25:43933113

  • Result on the web

    <a href="https://hdl.handle.net/11104/0369914" target="_blank" >https://hdl.handle.net/11104/0369914</a>

  • DOI - Digital Object Identifier

    <a href="http://dx.doi.org/10.1039/d5ra02009c" target="_blank" >10.1039/d5ra02009c</a>

Alternative languages

  • Result language

    angličtina

  • Original language name

    Biodegradable Zn-0.8Mg-0.2Sr alloy as an internal fixation material exhibits controlled degradation with enhanced osteogenesis

  • Original language description

    Zinc (Zn) and its alloys are promising candidates for biodegradable metals in medical applications. However, their clinical use in internal fixation is hindered by low mechanical strength, uncontrolled corrosion, and insufficient bioactivity. To address these issues, we developed an extruded Zn-0.8Mg-0.2Sr ternary alloy and systematically evaluated its biological performance. In vitro corrosion tests indicated that Zn-0.8Mg-0.2Sr exhibited superior corrosion resistance, attributed to a dense passivation layer that provided effective protection, controlled degradation kinetics, and milder Zn2+ release. The cytotoxicity of Zn-0.8Mg-0.2Sr toward pre-osteoblasts was concentration-dependent. Within the non-cytotoxic concentration range (Zn2+ ≤8.98 μg mL−1), Zn-0.8Mg-0.2Sr promoted osteogenic differentiation more effectively than pure Zn. Further in vivo studies confirmed favorable biocompatibility and more uniform degradation of Zn-0.8Mg-0.2Sr, with reduced pitting corrosion and structural collapse. Notably, Zn-0.8Mg-0.2Sr exhibited superior performance in promoting bone regeneration and anti-inflammatory immunomodulation compared to pure Zn. These findings highlight Zn-0.8Mg-0.2Sr as a promising alternative to conventional internal fixation materials, offering favorable biocompatibility, controlled biodegradability, and enhanced osteogenesis.

  • Czech name

  • Czech description

Classification

  • Type

    J<sub>imp</sub> - Article in a specialist periodical, which is included in the Web of Science database

  • CEP classification

  • OECD FORD branch

    10302 - Condensed matter physics (including formerly solid state physics, supercond.)

Result continuities

  • Project

    <a href="/en/project/GA23-05592S" target="_blank" >GA23-05592S: Influence of surface modifications on the functionality of zinc-based absorbable materials for applications in bone reconstructions</a><br>

  • Continuities

    I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace

Others

  • Publication year

    2025

  • Confidentiality

    S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů

Data specific for result type

  • Name of the periodical

    RSC Advances

  • ISSN

    2046-2069

  • e-ISSN

    2046-2069

  • Volume of the periodical

    15

  • Issue of the periodical within the volume

    37

  • Country of publishing house

    GB - UNITED KINGDOM

  • Number of pages

    18

  • Pages from-to

    30071-30088

  • UT code for WoS article

    001554775300001

  • EID of the result in the Scopus database

    2-s2.0-105013781736