The glass related properties of the SIBOR oxidation protective coating on molybdenum alloys
The result's identifiers
Result code in IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60461373%3A22310%2F08%3A00020482" target="_blank" >RIV/60461373:22310/08:00020482 - isvavai.cz</a>
Result on the web
—
DOI - Digital Object Identifier
—
Alternative languages
Result language
angličtina
Original language name
The glass related properties of the SIBOR oxidation protective coating on molybdenum alloys
Original language description
The SIBOR? (Si-10B-2C) oxidation protective coating was applied onto molybdenumand molybdenum ? 3 wt% zirconia samples by APS (= Atmospheric Plasma Spraying) with a subsequent heat treatment. Then the coated samples were submitted to ramp oxidation testswith heating rates of 10°C / hour up to a temperature of 1450°C. This procedure simulates the heating up of a glass melting tank where SIBOR? coated parts are most frequently used. Some of the samples which could be oxidized without any defect were thenimmersed in various molten glasses to determine the dissolution rate of the SIBOR? substrate system. This simulates the situation when the glass melting tank is filled and operated with molten glass. SIBOR? proved to be an excellent oxidation protectivecoating for the molybdenum ? zirconia ? material like for pure molybdenum. The coating was fairly good dissolved by opal glass and ? slightly less ? by soda lime glass. With borosilicate glass a much slower interaction was found. In all
Czech name
Vlasntosti skloviny mající vliv na ochrannou oxidační vrstvu SIBOR nanesenou na slitinách molybdenu
Czech description
Ochranná oxidační vrstva materiálu SIBOR (Si-10B-2C) byla použita na vzorky ze slitiny molybdenu a molybdenu s 3hm.% oxidu zirkoničitého. Vrstva byla nanesena metodou APS (Atmospheric Plasma Spraying) s následnou tepelnou dispozicí. Pak byly vzorky odeslány na testování odolnosti vůči oxidaci. Vzorky byly ohřívány rychlostí 10°C/hod až do teploty 1450°C. Tato procedura simuluje podmínky v reálné tavicí peci, kde je SIBOR jako ochranná vrstva často používán.
Classification
Type
J<sub>x</sub> - Unclassified - Peer-reviewed scientific article (Jimp, Jsc and Jost)
CEP classification
JH - Ceramics, fire-proof materials and glass
OECD FORD branch
—
Result continuities
Project
—
Continuities
Z - Vyzkumny zamer (s odkazem do CEZ)
Others
Publication year
2008
Confidentiality
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Data specific for result type
Name of the periodical
Advanced Materials Research
ISSN
1022-6680
e-ISSN
—
Volume of the periodical
—
Issue of the periodical within the volume
39-40
Country of publishing house
CH - SWITZERLAND
Number of pages
6
Pages from-to
—
UT code for WoS article
000257175200115