Hydrogen interaction with defects in ZnO
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216208%3A11320%2F13%3A10189468" target="_blank" >RIV/00216208:11320/13:10189468 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.4028/www.scientific.net/MSF.733.228" target="_blank" >http://dx.doi.org/10.4028/www.scientific.net/MSF.733.228</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.4028/www.scientific.net/MSF.733.228" target="_blank" >10.4028/www.scientific.net/MSF.733.228</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Hydrogen interaction with defects in ZnO
Popis výsledku v původním jazyce
In the present work hydrothermally grown ZnO single crystals were electrochemically charged with hydrogen. The influence of hydrogen on ZnO microstructure was investigated by positron annihilation spectroscopy (PAS) combined with X-ray diffraction (XRD)using synchrotron radiation. Hydrogen concentration in the samples was determined by nuclear reaction analysis (NRA). It was found that a high concentration of hydrogen can be introduced into ZnO by electrochemical loading. At low concentrations absorbedhydrogen causes elastic volume expansion of ZnO crystal. At higher concentration, hydrogen-induced stresses exceed the yield stress in ZnO and plastic deformation of the crystal takes place leading to formation a defected subsurface layer in the crystals.
Název v anglickém jazyce
Hydrogen interaction with defects in ZnO
Popis výsledku anglicky
In the present work hydrothermally grown ZnO single crystals were electrochemically charged with hydrogen. The influence of hydrogen on ZnO microstructure was investigated by positron annihilation spectroscopy (PAS) combined with X-ray diffraction (XRD)using synchrotron radiation. Hydrogen concentration in the samples was determined by nuclear reaction analysis (NRA). It was found that a high concentration of hydrogen can be introduced into ZnO by electrochemical loading. At low concentrations absorbedhydrogen causes elastic volume expansion of ZnO crystal. At higher concentration, hydrogen-induced stresses exceed the yield stress in ZnO and plastic deformation of the crystal takes place leading to formation a defected subsurface layer in the crystals.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JJ - Ostatní materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GAP108%2F11%2F0958" target="_blank" >GAP108/11/0958: Výzkum bodových defektů v ZnO a studium jejich interakce s vodíkem a dusíkem</a><br>
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)<br>S - Specificky vyzkum na vysokych skolach<br>I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2013
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Materials Science Forum
ISBN
—
ISSN
0255-5476
e-ISSN
—
Počet stran výsledku
4
Strana od-do
228-231
Název nakladatele
TRANS TECH PUBLICATIONS LTD
Místo vydání
STAFA-ZURICH
Místo konání akce
Smolenice
Datum konání akce
5. 9. 2011
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
000315535700047