Effect of Sintering on Defects in Yttria Stabilised Zirconia
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216208%3A11320%2F13%3A10189471" target="_blank" >RIV/00216208:11320/13:10189471 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.4028/www.scientific.net/MSF.733.236" target="_blank" >http://dx.doi.org/10.4028/www.scientific.net/MSF.733.236</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.4028/www.scientific.net/MSF.733.236" target="_blank" >10.4028/www.scientific.net/MSF.733.236</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Effect of Sintering on Defects in Yttria Stabilised Zirconia
Popis výsledku v původním jazyce
A variable energy slow positron beam was utilised to investigate depth dependent effects of sintering on the tetragonal yttria stabilised zirconia nanopowders. Positron implantation was combined with the determination of Doppler broadened profiles of annihilation radiation. The results are consistent with recent positron lifetime data showing that sintering at elevated temperatures leads to a disappearance of pores and a significant grain growth, which is demonstrated by a strong suppression of positronium formation and a substantial decrease in concentration of open volume defects at triple points, respectively, with increasing sintering temperature. An existence of a subsurface layer of a relatively high content of defects was shown in sintered samples and tentatively attributed to arise from a diffusion of open volume defects from the sample interior toward the surface or from a sintering-induced surface modification.
Název v anglickém jazyce
Effect of Sintering on Defects in Yttria Stabilised Zirconia
Popis výsledku anglicky
A variable energy slow positron beam was utilised to investigate depth dependent effects of sintering on the tetragonal yttria stabilised zirconia nanopowders. Positron implantation was combined with the determination of Doppler broadened profiles of annihilation radiation. The results are consistent with recent positron lifetime data showing that sintering at elevated temperatures leads to a disappearance of pores and a significant grain growth, which is demonstrated by a strong suppression of positronium formation and a substantial decrease in concentration of open volume defects at triple points, respectively, with increasing sintering temperature. An existence of a subsurface layer of a relatively high content of defects was shown in sintered samples and tentatively attributed to arise from a diffusion of open volume defects from the sample interior toward the surface or from a sintering-induced surface modification.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JH - Keramika, žáruvzdorné materiály a skla
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)<br>I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2013
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Materials Science Forum
ISBN
—
ISSN
0255-5476
e-ISSN
—
Počet stran výsledku
4
Strana od-do
236-239
Název nakladatele
TRANS TECH PUBLICATIONS LTD
Místo vydání
STAFA-ZURICH
Místo konání akce
Smolenice
Datum konání akce
5. 9. 2011
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
000315535700049