Microstructure evolution in solution treated Ti15Mo alloy processed by high pressure torsion
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216208%3A11320%2F14%3A10287949" target="_blank" >RIV/00216208:11320/14:10287949 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.matchar.2014.10.024" target="_blank" >http://dx.doi.org/10.1016/j.matchar.2014.10.024</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.matchar.2014.10.024" target="_blank" >10.1016/j.matchar.2014.10.024</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Microstructure evolution in solution treated Ti15Mo alloy processed by high pressure torsion
Popis výsledku v původním jazyce
Microstructure evolution and mechanical properties of ultra-fine grained Ti15Mo alloy processed by high pressure torsion were investigated. High pressure torsion straining resulted in strong grain refinement as-observed by transmission electron microscopy. Microhardness and light microscopy showed two distinct regions-(i) a central region with radial material flow and low microhardness (340 HV) and (ii) a peripheral region with rotational material flow and high microhardness (430 HV). Positron annihilation spectroscopy showed that the only detectable defects in the material are dislocations, whose density increases with the radial distance and the number of high pressure torsion revolutions. The local chemical environment around defects does not differsignificantly from the average composition. (C) 2014 Elsevier Inc. All rights reserved.
Název v anglickém jazyce
Microstructure evolution in solution treated Ti15Mo alloy processed by high pressure torsion
Popis výsledku anglicky
Microstructure evolution and mechanical properties of ultra-fine grained Ti15Mo alloy processed by high pressure torsion were investigated. High pressure torsion straining resulted in strong grain refinement as-observed by transmission electron microscopy. Microhardness and light microscopy showed two distinct regions-(i) a central region with radial material flow and low microhardness (340 HV) and (ii) a peripheral region with rotational material flow and high microhardness (430 HV). Positron annihilation spectroscopy showed that the only detectable defects in the material are dislocations, whose density increases with the radial distance and the number of high pressure torsion revolutions. The local chemical environment around defects does not differsignificantly from the average composition. (C) 2014 Elsevier Inc. All rights reserved.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
BM - Fyzika pevných látek a magnetismus
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach<br>I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2014
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Materials Characterization
ISSN
1044-5803
e-ISSN
—
Svazek periodika
98
Číslo periodika v rámci svazku
-
Stát vydavatele periodika
US - Spojené státy americké
Počet stran výsledku
8
Strana od-do
233-240
Kód UT WoS článku
000347588700030
EID výsledku v databázi Scopus
—