Nanocrystalline aluminium particles inside Mg-4Li-4Al-2RE magnesium alloy after severe plastic deformation
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216208%3A11320%2F17%3A10369908" target="_blank" >RIV/00216208:11320/17:10369908 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.matchar.2016.12.021" target="_blank" >http://dx.doi.org/10.1016/j.matchar.2016.12.021</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.matchar.2016.12.021" target="_blank" >10.1016/j.matchar.2016.12.021</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Nanocrystalline aluminium particles inside Mg-4Li-4Al-2RE magnesium alloy after severe plastic deformation
Popis výsledku v původním jazyce
Detailed microstructure characterization of ultra-fine grained LAE442 magnesium alloy processed by ECAP was performed by transmission electron microscopy and positron annihilation spectroscopy. Formation of FCC aluminium particles in the magnesium matrix and intensive segregation of aluminium at dislocations was observed. In situ annealing in the transmission electron microscope together with the analysis of the positron annihilation spectrum showed the limited stability of Al particles and Al segregation at temperatures below the processing temperature. It was suggested that the formation of observed Al nanoparticles is caused by the synergic effect of high external stresses during ECAP and the presence of Li atoms dissolved in the Mg matrix.
Název v anglickém jazyce
Nanocrystalline aluminium particles inside Mg-4Li-4Al-2RE magnesium alloy after severe plastic deformation
Popis výsledku anglicky
Detailed microstructure characterization of ultra-fine grained LAE442 magnesium alloy processed by ECAP was performed by transmission electron microscopy and positron annihilation spectroscopy. Formation of FCC aluminium particles in the magnesium matrix and intensive segregation of aluminium at dislocations was observed. In situ annealing in the transmission electron microscope together with the analysis of the positron annihilation spectrum showed the limited stability of Al particles and Al segregation at temperatures below the processing temperature. It was suggested that the formation of observed Al nanoparticles is caused by the synergic effect of high external stresses during ECAP and the presence of Li atoms dissolved in the Mg matrix.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
10302 - Condensed matter physics (including formerly solid state physics, supercond.)
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2017
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Materials Characterization
ISSN
1044-5803
e-ISSN
—
Svazek periodika
127
Číslo periodika v rámci svazku
neuveden
Stát vydavatele periodika
US - Spojené státy americké
Počet stran výsledku
5
Strana od-do
248-252
Kód UT WoS článku
000404817000031
EID výsledku v databázi Scopus
—