Study of the Resistances of Organic Coatings to Filiform Corrosion.
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216275%3A25310%2F02%3A00000275" target="_blank" >RIV/00216275:25310/02:00000275 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Study of the Resistances of Organic Coatings to Filiform Corrosion.
Popis výsledku v původním jazyce
The filiform corrosion is a special-type atmospheric corrosion, which broadens below the organic coatings and is characterized by its manifestation in the form of fibers or filaments. The appearance of this corrosion attack depends on several factors whimedium moisture and at the same time the presence of compouds stimulating the corrosion, such as chlorides, sulphates, acetates and further general factors supporting the atmospheric-corrosion appearance. The conditions of formation of this corrosion athigh relative humidity under simultaneous contamination of the substrate metal with soluble impurities such as sulfur dioxide, sulfates, chlorides, acetates. An important factor for broadening the filiform corrosion involves also the barrier or chemicalthe modes of filiform-corrosion initation and evaluation thereof under nonpigmented organic coatings based on various bidner bases. Also the possibility of retardation of the filiform corrosion by means of zinc powder and the effects of l
Název v anglickém jazyce
Study of the Resistances of Organic Coatings to Filiform Corrosion.
Popis výsledku anglicky
The filiform corrosion is a special-type atmospheric corrosion, which broadens below the organic coatings and is characterized by its manifestation in the form of fibers or filaments. The appearance of this corrosion attack depends on several factors whimedium moisture and at the same time the presence of compouds stimulating the corrosion, such as chlorides, sulphates, acetates and further general factors supporting the atmospheric-corrosion appearance. The conditions of formation of this corrosion athigh relative humidity under simultaneous contamination of the substrate metal with soluble impurities such as sulfur dioxide, sulfates, chlorides, acetates. An important factor for broadening the filiform corrosion involves also the barrier or chemicalthe modes of filiform-corrosion initation and evaluation thereof under nonpigmented organic coatings based on various bidner bases. Also the possibility of retardation of the filiform corrosion by means of zinc powder and the effects of l
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JK - Koroze a povrchové úpravy materiálu
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2002
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Acta Mechanica Slovaca
ISSN
1355-2393
e-ISSN
—
Svazek periodika
6
Číslo periodika v rámci svazku
2
Stát vydavatele periodika
SK - Slovenská republika
Počet stran výsledku
6
Strana od-do
93-98