Thermal properties and stability of TeO2 containing phosphate glasses
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216275%3A25310%2F11%3A39892076" target="_blank" >RIV/00216275:25310/11:39892076 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.tca.2011.01.020" target="_blank" >http://dx.doi.org/10.1016/j.tca.2011.01.020</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.tca.2011.01.020" target="_blank" >10.1016/j.tca.2011.01.020</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Thermal properties and stability of TeO2 containing phosphate glasses
Popis výsledku v původním jazyce
Differential thermal analysis and thermodilatometry have been used to study the thermal behaviour of glasses in the ZnO-P2O5-TeO2 system prepared in compositional series(100?x)[0.5ZnO-0.5P2O5]-xTeO2 (X-series) and 50ZnO-50?y)P2O5-yTeO2 (Y-series) withinthe concentration range of x = 0-60 and y = 0 40 mol% TeO2. The addition of TeO2 to the starting zinc metaphosphate glass resulted in a gradual increase of thermal expansion coefficient from 12.2 up to 16.6 ppm?C?1, whereas glass transition temperature and dilatometric softening temperature reveal a minimum at the glass with x = 30 mol% and y = 10 mol % TeO2. All glasses crystallize on heating within the temperature range ?500-700 ?C. The contribution of the surface crystallization mechanism over the internal one increases with increasing TeO2 content. Major compounds formed by crystallization were Zn(PO3)2 and Zn2P2O7.
Název v anglickém jazyce
Thermal properties and stability of TeO2 containing phosphate glasses
Popis výsledku anglicky
Differential thermal analysis and thermodilatometry have been used to study the thermal behaviour of glasses in the ZnO-P2O5-TeO2 system prepared in compositional series(100?x)[0.5ZnO-0.5P2O5]-xTeO2 (X-series) and 50ZnO-50?y)P2O5-yTeO2 (Y-series) withinthe concentration range of x = 0-60 and y = 0 40 mol% TeO2. The addition of TeO2 to the starting zinc metaphosphate glass resulted in a gradual increase of thermal expansion coefficient from 12.2 up to 16.6 ppm?C?1, whereas glass transition temperature and dilatometric softening temperature reveal a minimum at the glass with x = 30 mol% and y = 10 mol % TeO2. All glasses crystallize on heating within the temperature range ?500-700 ?C. The contribution of the surface crystallization mechanism over the internal one increases with increasing TeO2 content. Major compounds formed by crystallization were Zn(PO3)2 and Zn2P2O7.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
CA - Anorganická chemie
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GAP106%2F10%2F0283" target="_blank" >GAP106/10/0283: Ternární fosfátová skla dotovaná oxidy přechodných kovů pro optoelektronické aplikace</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>Z - Vyzkumny zamer (s odkazem do CEZ)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2011
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Thermochimica Acta
ISSN
0040-6031
e-ISSN
—
Svazek periodika
522
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
NL - Nizozemsko
Počet stran výsledku
6
Strana od-do
155-160
Kód UT WoS článku
000294593900022