Soda Pulp Cooked From Rapeseed Straw
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216275%3A25310%2F16%3A39901675" target="_blank" >RIV/00216275:25310/16:39901675 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Soda Pulp Cooked From Rapeseed Straw
Popis výsledku v původním jazyce
The paper deals with batch soda cooking of pulp from rapeseed straw. The preliminary runs were focused on determination of active alkali charge and liquor-to-straw ratio upon the delignification degree of pulp. For suitable cooking parameters, viz. active alkali charge of 19 %, liquor-to-straw ratio of 5:1, and anthraquinone charge of 0.1 %, the effect of the delignification degree directly proportional to the H-factor upon the total yield, kappa number, and amount of rejects was investigated in the H-factor interval from 800 to 2,800 h. For soda-AQ cooks of straw, stalks, and silique valves, the total pulp yield, kappa number, as well as amount of rejects decreased with increasing H-factor. The greatest total yield and degree of delignification were found for soda-AQ pulp cooked from stalks only. On the contrary, the silique valves gave the lowest total yield. The degree of polymerisation of pulp cooked from straw, stalks, and silique valves increased with increasing H-factor, the greatest values were measured for pulp from stalks. The colour properties of pulp from straw and stalks including brightness found in the interval of 30 to 34 did not differ significantly each other. However, the tensile strength of handsheets made of pulp once dried and repulped was found to be markedly lower in comparison with never dried pulp.
Název v anglickém jazyce
Soda Pulp Cooked From Rapeseed Straw
Popis výsledku anglicky
The paper deals with batch soda cooking of pulp from rapeseed straw. The preliminary runs were focused on determination of active alkali charge and liquor-to-straw ratio upon the delignification degree of pulp. For suitable cooking parameters, viz. active alkali charge of 19 %, liquor-to-straw ratio of 5:1, and anthraquinone charge of 0.1 %, the effect of the delignification degree directly proportional to the H-factor upon the total yield, kappa number, and amount of rejects was investigated in the H-factor interval from 800 to 2,800 h. For soda-AQ cooks of straw, stalks, and silique valves, the total pulp yield, kappa number, as well as amount of rejects decreased with increasing H-factor. The greatest total yield and degree of delignification were found for soda-AQ pulp cooked from stalks only. On the contrary, the silique valves gave the lowest total yield. The degree of polymerisation of pulp cooked from straw, stalks, and silique valves increased with increasing H-factor, the greatest values were measured for pulp from stalks. The colour properties of pulp from straw and stalks including brightness found in the interval of 30 to 34 did not differ significantly each other. However, the tensile strength of handsheets made of pulp once dried and repulped was found to be markedly lower in comparison with never dried pulp.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JJ - Ostatní materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2016
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Cellulose Chemistry and Technology
ISSN
0576-9787
e-ISSN
—
Svazek periodika
50
Číslo periodika v rámci svazku
5-6
Stát vydavatele periodika
RO - Rumunsko
Počet stran výsledku
8
Strana od-do
681-688
Kód UT WoS článku
000386993700021
EID výsledku v databázi Scopus
—