Ageing of Ge24.9Sb11.6S63.5 thin films under various conditions
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216275%3A25310%2F17%3A39911195" target="_blank" >RIV/00216275:25310/17:39911195 - isvavai.cz</a>
Výsledek na webu
<a href="http://www.sciencedirect.com/science/article/pii/S0254058417302924" target="_blank" >http://www.sciencedirect.com/science/article/pii/S0254058417302924</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.matchemphys.2017.04.019" target="_blank" >10.1016/j.matchemphys.2017.04.019</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Ageing of Ge24.9Sb11.6S63.5 thin films under various conditions
Popis výsledku v původním jazyce
Amorphous Ge24.9Sb11.6S63.5 thin films prepared by thermal evaporation were aged for more than 1 year under various conditions: in the dark in a desiccator, in a dark and humid atmosphere and under laboratory conditions under daylight. The bleaching of thin films (the blue shift of the optical band gap) was observed with the magnitude depending on the storage conditions. The photo-sensitivity of the aged thin films was significantly affected by storage conditions and was found to decrease with the increasing time of ageing. The changes in thin films during the ageing were monitored with respect to the chemical composition, the structure, the surface wettability, the surface topology and information about the depth and optical parameters of the formed over-layer and were finally correlated with the storage conditions.
Název v anglickém jazyce
Ageing of Ge24.9Sb11.6S63.5 thin films under various conditions
Popis výsledku anglicky
Amorphous Ge24.9Sb11.6S63.5 thin films prepared by thermal evaporation were aged for more than 1 year under various conditions: in the dark in a desiccator, in a dark and humid atmosphere and under laboratory conditions under daylight. The bleaching of thin films (the blue shift of the optical band gap) was observed with the magnitude depending on the storage conditions. The photo-sensitivity of the aged thin films was significantly affected by storage conditions and was found to decrease with the increasing time of ageing. The changes in thin films during the ageing were monitored with respect to the chemical composition, the structure, the surface wettability, the surface topology and information about the depth and optical parameters of the formed over-layer and were finally correlated with the storage conditions.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
10402 - Inorganic and nuclear chemistry
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2017
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Materials Chemistry and Physics
ISSN
0254-0584
e-ISSN
—
Svazek periodika
195
Číslo periodika v rámci svazku
July
Stát vydavatele periodika
CH - Švýcarská konfederace
Počet stran výsledku
11
Strana od-do
236-246
Kód UT WoS článku
000402218400030
EID výsledku v databázi Scopus
—