Effect of primary driers on oxidative drying of high-solid alkyd binder: Investigation of thickness effects by mechanical tests and infrared spectroscopy
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216275%3A25310%2F18%3A39912975" target="_blank" >RIV/00216275:25310/18:39912975 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.porgcoat.2018.09.001" target="_blank" >http://dx.doi.org/10.1016/j.porgcoat.2018.09.001</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.porgcoat.2018.09.001" target="_blank" >10.1016/j.porgcoat.2018.09.001</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Effect of primary driers on oxidative drying of high-solid alkyd binder: Investigation of thickness effects by mechanical tests and infrared spectroscopy
Popis výsledku v původním jazyce
Catalytic activity of four primary driers was investigated in high-solid alkyd binder modified with tall oil fatty acids. The drying activity was established by mechanical tests. Infrared spectroscopy was used for detailed investigation of chemical changes during the autoxidation process. Due to strong thickness effect, the infrared study was performed using attenuated total reflectance (ATR) technique, which measures spectra of a thin layer from the interface sample/ATR crystal (down surface of the sample). Coatings of 30-wet thickness were found to be enough thin to be considered as a homogenously dried bulk with negligible effect of oxygen diffusion. It makes the 30-layers very suitable for determination of kinetic parameters of the autoxidation process. For the first time, ATR-IR experiments on several samples of the same composition but different film thickness were used for detailed investigation of the thickness effect.
Název v anglickém jazyce
Effect of primary driers on oxidative drying of high-solid alkyd binder: Investigation of thickness effects by mechanical tests and infrared spectroscopy
Popis výsledku anglicky
Catalytic activity of four primary driers was investigated in high-solid alkyd binder modified with tall oil fatty acids. The drying activity was established by mechanical tests. Infrared spectroscopy was used for detailed investigation of chemical changes during the autoxidation process. Due to strong thickness effect, the infrared study was performed using attenuated total reflectance (ATR) technique, which measures spectra of a thin layer from the interface sample/ATR crystal (down surface of the sample). Coatings of 30-wet thickness were found to be enough thin to be considered as a homogenously dried bulk with negligible effect of oxygen diffusion. It makes the 30-layers very suitable for determination of kinetic parameters of the autoxidation process. For the first time, ATR-IR experiments on several samples of the same composition but different film thickness were used for detailed investigation of the thickness effect.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20506 - Coating and films
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2018
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Progress in Organic Coatings
ISSN
0300-9440
e-ISSN
—
Svazek periodika
125
Číslo periodika v rámci svazku
December
Stát vydavatele periodika
NL - Nizozemsko
Počet stran výsledku
9
Strana od-do
177-185
Kód UT WoS článku
000453642900021