Study on Mechanical Properties of Heap Deposited Fly Ash Based Geopolymers with Different Alkaline Activator Properties
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26110%2F22%3APU146013" target="_blank" >RIV/00216305:26110/22:PU146013 - isvavai.cz</a>
Výsledek na webu
<a href="https://www.mdpi.com/2075-5309/12/11/1780" target="_blank" >https://www.mdpi.com/2075-5309/12/11/1780</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.3390/buildings12111780" target="_blank" >10.3390/buildings12111780</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Study on Mechanical Properties of Heap Deposited Fly Ash Based Geopolymers with Different Alkaline Activator Properties
Popis výsledku v původním jazyce
Geopolymers can improve environmental protection and are therefore considered a 21st-century material that requires special attention. The main objective of this study was to examine the utilization of fly ash deposited on a heap as a potential raw material for the geopolymerization process. In this work, flexural and compressive strengths, as well as water absorption of geopolymers, were evaluated based on alkaline activator properties. Na2O content, SiO2/Na2O molar ratio and fly ash-to-water ratio were key observed factors. Mechanical strengths tests were conducted after 7, 28, 90, 180, and 360 days. The research findings showed that geopolymer cured at appropriate conditions and with a suitable alkaline activator can reach a compressive strength of more than 55 MPa. The presented study highlighted the possibility of the efficient use of fly ash to produce useful materials, i.e., geopolymers, which contribute to environmentally friendly solutions. This approach is fully in line with the principles of sustainable development.
Název v anglickém jazyce
Study on Mechanical Properties of Heap Deposited Fly Ash Based Geopolymers with Different Alkaline Activator Properties
Popis výsledku anglicky
Geopolymers can improve environmental protection and are therefore considered a 21st-century material that requires special attention. The main objective of this study was to examine the utilization of fly ash deposited on a heap as a potential raw material for the geopolymerization process. In this work, flexural and compressive strengths, as well as water absorption of geopolymers, were evaluated based on alkaline activator properties. Na2O content, SiO2/Na2O molar ratio and fly ash-to-water ratio were key observed factors. Mechanical strengths tests were conducted after 7, 28, 90, 180, and 360 days. The research findings showed that geopolymer cured at appropriate conditions and with a suitable alkaline activator can reach a compressive strength of more than 55 MPa. The presented study highlighted the possibility of the efficient use of fly ash to produce useful materials, i.e., geopolymers, which contribute to environmentally friendly solutions. This approach is fully in line with the principles of sustainable development.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2022
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Buildings
ISSN
2075-5309
e-ISSN
—
Svazek periodika
12
Číslo periodika v rámci svazku
11
Stát vydavatele periodika
CH - Švýcarská konfederace
Počet stran výsledku
14
Strana od-do
1-14
Kód UT WoS článku
000880984600001