Spolehlivost keramické hlavice totální kyčelní endoporotézy určená pomocí Weibullovy teorie nejslabšího článku
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26210%2F06%3APU63159" target="_blank" >RIV/00216305:26210/06:PU63159 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/61388998:_____/06:00044148
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Reliability of the Ceramic Head of the Total Hip Joint Endoprosthesis Using Weibull's Weakest-link Theory
Popis výsledku v původním jazyce
The paper deals with calculation of the parameters of ceramic material from a set of destruction tests of ceramic heads of total hip joint endoprosthesis. The standard way of calculation of the material parameters consists in carrying out a set of 3 or 4point bending tests of specimens cut out from parts of the ceramic material to be analysed. In case of ceramic heads, it is not possible to cut out specimens of required dimensions because the heads are too small (if the cut out specimens were smaller than the normalised ones, the material parameters derived from them would exhibit higher strength values than those which the given ceramic material really has). On that score, a special testing jig was made, in which 40 heads were destructed. From the measured values of circumferential strains of the head's external spherical surface under destruction, the state of stress in the head under destruction was established using the final elements method (FEM). From the values obtained, the so
Název v anglickém jazyce
Reliability of the Ceramic Head of the Total Hip Joint Endoprosthesis Using Weibull's Weakest-link Theory
Popis výsledku anglicky
The paper deals with calculation of the parameters of ceramic material from a set of destruction tests of ceramic heads of total hip joint endoprosthesis. The standard way of calculation of the material parameters consists in carrying out a set of 3 or 4point bending tests of specimens cut out from parts of the ceramic material to be analysed. In case of ceramic heads, it is not possible to cut out specimens of required dimensions because the heads are too small (if the cut out specimens were smaller than the normalised ones, the material parameters derived from them would exhibit higher strength values than those which the given ceramic material really has). On that score, a special testing jig was made, in which 40 heads were destructed. From the measured values of circumferential strains of the head's external spherical surface under destruction, the state of stress in the head under destruction was established using the final elements method (FEM). From the values obtained, the so
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
BO - Biofyzika
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GP101%2F04%2FP037" target="_blank" >GP101/04/P037: Zvýšení úrovně výpočtového modelování pro určování pravděpodobnosti porušení keramické hlavice kyčelní endoprotézy</a><br>
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2006
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
World Congress on Medical Physics and Biomedical engineering 2006
ISBN
3-540-36839-6
ISSN
—
e-ISSN
—
Počet stran výsledku
4
Strana od-do
2818-2821
Název nakladatele
Springer
Místo vydání
Seoul
Místo konání akce
Seoul
Datum konání akce
27. 8. 2006
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—