MAPPING OF FILM THICKNESS IN BOVINE SERUM LUBRICATED CONTACTS
Popis výsledku v původním jazyce
The aim of this study is to perform detail experimental mapping of the lubricating film thickness of bovine serum (BS) within the contact between an artificial metal or ceramic femoral head and a glass disc and analyze effect of proteins on the film formation. Mapping of the lubricating film of various concentrations of BS solutions was carried out using an optical test rig. Chromatic interferograms were recorded with a high-speed digital camera and evaluated with thin film colorimetric interferometry.The film thickness was studied as a function of both time and mean speed. The results showed that film thickness increases with time for both the metal and ceramic heads. Films formed at the end of measurements with the metal head were found to be typically in the range of 60?100 nm for all BS solutions and were independent on the amount of proteins in tested fluids. At the beginning of the speed measurements, BS of all concentrations forms a very thin film (1?2 nm) and its thickness inc
Název v anglickém jazyce
MAPPING OF FILM THICKNESS IN BOVINE SERUM LUBRICATED CONTACTS
Popis výsledku anglicky
The aim of this study is to perform detail experimental mapping of the lubricating film thickness of bovine serum (BS) within the contact between an artificial metal or ceramic femoral head and a glass disc and analyze effect of proteins on the film formation. Mapping of the lubricating film of various concentrations of BS solutions was carried out using an optical test rig. Chromatic interferograms were recorded with a high-speed digital camera and evaluated with thin film colorimetric interferometry.The film thickness was studied as a function of both time and mean speed. The results showed that film thickness increases with time for both the metal and ceramic heads. Films formed at the end of measurements with the metal head were found to be typically in the range of 60?100 nm for all BS solutions and were independent on the amount of proteins in tested fluids. At the beginning of the speed measurements, BS of all concentrations forms a very thin film (1?2 nm) and its thickness inc
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JR - Ostatní strojírenství
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/ED0002%2F01%2F01" target="_blank" >ED0002/01/01: NETME Centre (Nové technologie pro strojírenství)</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2013
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Engineering Mechanics
ISSN
1802-1484
e-ISSN
—
Svazek periodika
20
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
15
Strana od-do
27-41
Kód UT WoS článku
—
EID výsledku v databázi Scopus
—