Changes in structure and in mechanical properties during the pyrolysis conversion of crosslinked polymethylsiloxane and polymethylphenilsiloxane resins to silicon oxycarbide glass
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26210%2F15%3APU113466" target="_blank" >RIV/00216305:26210/15:PU113466 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.ceramint.2015.01.034" target="_blank" >http://dx.doi.org/10.1016/j.ceramint.2015.01.034</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.ceramint.2015.01.034" target="_blank" >10.1016/j.ceramint.2015.01.034</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Changes in structure and in mechanical properties during the pyrolysis conversion of crosslinked polymethylsiloxane and polymethylphenilsiloxane resins to silicon oxycarbide glass
Popis výsledku v původním jazyce
The subject of this study is the thermally induced conversion of cross-linked polymethylsiloxane and polymethylphenylsiloxane resins into inorganic silicon oxycarbide glass. This topic is studied in view of the changes in the chemical structure of the precursor and in the context of the changes in hardness and elasticity, pyrolysis weight losses, density changes, and sample shrinkage. Two aspects of the pyrolysis process were studied: i) the effect of the pyrolysis temperature (tested from 400 to 1000C) and ii) the effect of pyrolysis time in cases of isothermal pyrolyses (at 520C and 650C). The mechanical properties were evaluated by means of micro-indentation tests, while the characterisation of the chemical structure was performed via FTIR spectroscopy, combustion analysis and EDS. The results of these experiments are discussed in the context of the use of examined materials as a precursor for the composite matrix or the sandwich core.
Název v anglickém jazyce
Changes in structure and in mechanical properties during the pyrolysis conversion of crosslinked polymethylsiloxane and polymethylphenilsiloxane resins to silicon oxycarbide glass
Popis výsledku anglicky
The subject of this study is the thermally induced conversion of cross-linked polymethylsiloxane and polymethylphenylsiloxane resins into inorganic silicon oxycarbide glass. This topic is studied in view of the changes in the chemical structure of the precursor and in the context of the changes in hardness and elasticity, pyrolysis weight losses, density changes, and sample shrinkage. Two aspects of the pyrolysis process were studied: i) the effect of the pyrolysis temperature (tested from 400 to 1000C) and ii) the effect of pyrolysis time in cases of isothermal pyrolyses (at 520C and 650C). The mechanical properties were evaluated by means of micro-indentation tests, while the characterisation of the chemical structure was performed via FTIR spectroscopy, combustion analysis and EDS. The results of these experiments are discussed in the context of the use of examined materials as a precursor for the composite matrix or the sandwich core.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20504 - Ceramics
Návaznosti výsledku
Projekt
—
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2015
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Ceramics International
ISSN
0272-8842
e-ISSN
1873-3956
Svazek periodika
41
Číslo periodika v rámci svazku
5
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
11
Strana od-do
6237-6247
Kód UT WoS článku
000353176300013
EID výsledku v databázi Scopus
2-s2.0-84925355081