Overcooling in overlap areas during hydraulic Descaling
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26210%2F16%3APU119879" target="_blank" >RIV/00216305:26210/16:PU119879 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.17222/mit.2015.164" target="_blank" >http://dx.doi.org/10.17222/mit.2015.164</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.17222/mit.2015.164" target="_blank" >10.17222/mit.2015.164</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Overcooling in overlap areas during hydraulic Descaling
Popis výsledku v původním jazyce
The production and processing of high-quality grades of steel are connected with the oxidation at high temperatures. Unwanted scales are formed on the steel surface, which is usually heated to over 900 °C. These scales are often removed by hydraulic descaling during the production. In most cases where long, flat products are produced, one row of descaling nozzles is used. As these flat jet nozzles are arranged in a row, the water spray from one nozzle interferes with the spray from the neighboring nozzles. This zone is called an overlap area and often even more scales remain here after the descaling process. An increased amount of the scales left behind results in a lower quality of a final product. A typical configuration with an inclination and twist angle of 15° was studied. Heat-transfer coefficients (HTC) and surface temperatures were measured in the overlap area and compared with the values obtained from undisturbed areas. It was found that the overlap area is grossly overcooled. The results were compared with a new configuration, where the twist angle was changed to 0°, and it was found that the overcooling was significantly reduced. The temperature measurement showed that an increased thickness of the scales in the overlap area can also be caused by surface overcooling because the scales change the material properties with the temperature, and they are therefore more difficult to remove. The new configuration with the twist angle of 0° seems promising for improving the quality of hydraulic descaling.
Název v anglickém jazyce
Overcooling in overlap areas during hydraulic Descaling
Popis výsledku anglicky
The production and processing of high-quality grades of steel are connected with the oxidation at high temperatures. Unwanted scales are formed on the steel surface, which is usually heated to over 900 °C. These scales are often removed by hydraulic descaling during the production. In most cases where long, flat products are produced, one row of descaling nozzles is used. As these flat jet nozzles are arranged in a row, the water spray from one nozzle interferes with the spray from the neighboring nozzles. This zone is called an overlap area and often even more scales remain here after the descaling process. An increased amount of the scales left behind results in a lower quality of a final product. A typical configuration with an inclination and twist angle of 15° was studied. Heat-transfer coefficients (HTC) and surface temperatures were measured in the overlap area and compared with the values obtained from undisturbed areas. It was found that the overlap area is grossly overcooled. The results were compared with a new configuration, where the twist angle was changed to 0°, and it was found that the overcooling was significantly reduced. The temperature measurement showed that an increased thickness of the scales in the overlap area can also be caused by surface overcooling because the scales change the material properties with the temperature, and they are therefore more difficult to remove. The new configuration with the twist angle of 0° seems promising for improving the quality of hydraulic descaling.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
<a href="/cs/project/LO1202" target="_blank" >LO1202: NETME CENTRE PLUS</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2016
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Materiali in tehnologije
ISSN
1580-2949
e-ISSN
1580-3414
Svazek periodika
50
Číslo periodika v rámci svazku
4
Stát vydavatele periodika
SI - Slovinská republika
Počet stran výsledku
4
Strana od-do
575-578
Kód UT WoS článku
000381658000019
EID výsledku v databázi Scopus
2-s2.0-84983637813