Abrasion of Magnetorheological Fluids
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26210%2F19%3APU132201" target="_blank" >RIV/00216305:26210/19:PU132201 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.21495/71-0-169" target="_blank" >http://dx.doi.org/10.21495/71-0-169</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.21495/71-0-169" target="_blank" >10.21495/71-0-169</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Abrasion of Magnetorheological Fluids
Popis výsledku v původním jazyce
This paper deals with the study of the abrasive effect of commercial magnetorheological (MR) fluids on steel material. The tests were performed on a tribometer with a pin-on-plate configuration; the sample was flooded with the examined fluid. The rate of abrasion, caused by MR fluids and hydraulic oil, was compared. The difference among the tested MR fluids has been shown to be minimal and the abrasion is approximately twice as large as when using hydraulic oil. The results are beneficial for the development of MR dampers, a material with a higher resistance against abrasion wear must be used for a hydraulic tube. Furthermore, the testing procedure and test conditions were established and thus this test can be repeated with new materials until the abrasion is not as extensive as that with hydraulic oil.
Název v anglickém jazyce
Abrasion of Magnetorheological Fluids
Popis výsledku anglicky
This paper deals with the study of the abrasive effect of commercial magnetorheological (MR) fluids on steel material. The tests were performed on a tribometer with a pin-on-plate configuration; the sample was flooded with the examined fluid. The rate of abrasion, caused by MR fluids and hydraulic oil, was compared. The difference among the tested MR fluids has been shown to be minimal and the abrasion is approximately twice as large as when using hydraulic oil. The results are beneficial for the development of MR dampers, a material with a higher resistance against abrasion wear must be used for a hydraulic tube. Furthermore, the testing procedure and test conditions were established and thus this test can be repeated with new materials until the abrasion is not as extensive as that with hydraulic oil.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
—
OECD FORD obor
20302 - Applied mechanics
Návaznosti výsledku
Projekt
<a href="/cs/project/GC17-10660J" target="_blank" >GC17-10660J: Výzkum magnetoreologické kapaliny s vysokou sedimentační stabilitou</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2019
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Engineering Mechanics 2019, 25th International Conference
ISBN
978-80-87012-71-0
ISSN
—
e-ISSN
—
Počet stran výsledku
4
Strana od-do
169-172
Název nakladatele
Institute of Thermomechanics of the Czech Academy of Sciences
Místo vydání
Praha
Místo konání akce
Svratka
Datum konání akce
13. 5. 2019
Typ akce podle státní příslušnosti
EUR - Evropská akce
Kód UT WoS článku