Middle stage of Portland cement hydration influenced by different portions of silica fume, metakaolin and ground granulated blast-furnace slag
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26310%2F19%3APU134274" target="_blank" >RIV/00216305:26310/19:PU134274 - isvavai.cz</a>
Výsledek na webu
<a href="https://link.springer.com/article/10.1007/s10973-019-08313-6" target="_blank" >https://link.springer.com/article/10.1007/s10973-019-08313-6</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1007/s10973-019-08313-6" target="_blank" >10.1007/s10973-019-08313-6</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Middle stage of Portland cement hydration influenced by different portions of silica fume, metakaolin and ground granulated blast-furnace slag
Popis výsledku v původním jazyce
Present study deals with the influence of metakaolin (MK), silica fume (SF) and ground granulated blast-furnace slag (BFS) on middle hydration of ordinary Portland cement replaced by 45 mass% of particular supplementary cementitious materials (SCMs). Acceleration of cement hydration by SF and MK was proved up to the first 12 h by isothermal calorimetry as well as by thermogravimetric analyses. From the beginning of deceleratory period, when SCMs stopped to act as accelerators, more evident influence of the dilution effect was observed. Nevertheless, the presence of pozzolanic reactions was demonstrated already after 15 h of curing and even when SF and MK were used in the amount equal to 5 mass%. Synergic effect of the used SCMs allowed to increase the quantity of BFS up to 35 mass% without significant changes in their positive action.
Název v anglickém jazyce
Middle stage of Portland cement hydration influenced by different portions of silica fume, metakaolin and ground granulated blast-furnace slag
Popis výsledku anglicky
Present study deals with the influence of metakaolin (MK), silica fume (SF) and ground granulated blast-furnace slag (BFS) on middle hydration of ordinary Portland cement replaced by 45 mass% of particular supplementary cementitious materials (SCMs). Acceleration of cement hydration by SF and MK was proved up to the first 12 h by isothermal calorimetry as well as by thermogravimetric analyses. From the beginning of deceleratory period, when SCMs stopped to act as accelerators, more evident influence of the dilution effect was observed. Nevertheless, the presence of pozzolanic reactions was demonstrated already after 15 h of curing and even when SF and MK were used in the amount equal to 5 mass%. Synergic effect of the used SCMs allowed to increase the quantity of BFS up to 35 mass% without significant changes in their positive action.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
10402 - Inorganic and nuclear chemistry
Návaznosti výsledku
Projekt
<a href="/cs/project/LO1211" target="_blank" >LO1211: Centrum materiálového výzkumu na FCH VUT v Brně - udržitelnost a rozvoj</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2019
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Journal of Thermal Analysis and Calorimetry
ISSN
1388-6150
e-ISSN
1588-2926
Svazek periodika
138
Číslo periodika v rámci svazku
6
Stát vydavatele periodika
HU - Maďarsko
Počet stran výsledku
8
Strana od-do
4119-4126