PREPARATION OF PEO COATINGS ON AZ31 MAGNESIUM ALLOY IN THE PRESENCE OF HUMIC ACID
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26310%2F24%3APU154843" target="_blank" >RIV/00216305:26310/24:PU154843 - isvavai.cz</a>
Výsledek na webu
<a href="https://www.confer.cz/metal/2023/4713-preparation-of-peo-coatings-in-the-presence-of-humic-acid-on-az31-magnesium-alloy" target="_blank" >https://www.confer.cz/metal/2023/4713-preparation-of-peo-coatings-in-the-presence-of-humic-acid-on-az31-magnesium-alloy</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.37904/metal.2023.4713" target="_blank" >10.37904/metal.2023.4713</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
PREPARATION OF PEO COATINGS ON AZ31 MAGNESIUM ALLOY IN THE PRESENCE OF HUMIC ACID
Popis výsledku v původním jazyce
Magnesium materials are desirable for surface treatment because of their low corrosion resistance. The preparation of coatings on AZ31 alloy by plasma electrolytic oxidation (PEO) in a bath with and without humic acid was investigated. The coatings were characterized using a scanning electron microscope (SEM) with energy dispersive X-ray spectroscopy (EDS) and Fourier transform infrared spectroscopy (FTIR). The corrosion properties were tested using the potentiodynamic polarization method in 0.15 M NaCl. The results show that the PEO coatings had significantly higher corrosion resistance than the AZ31 alloy. The PEO coating prepared in the presence of 5 mg/l humic acid (10 min deposition) appeared to have slightly better corrosion resistance than the PEO coating prepared in the absence of humic acid.
Název v anglickém jazyce
PREPARATION OF PEO COATINGS ON AZ31 MAGNESIUM ALLOY IN THE PRESENCE OF HUMIC ACID
Popis výsledku anglicky
Magnesium materials are desirable for surface treatment because of their low corrosion resistance. The preparation of coatings on AZ31 alloy by plasma electrolytic oxidation (PEO) in a bath with and without humic acid was investigated. The coatings were characterized using a scanning electron microscope (SEM) with energy dispersive X-ray spectroscopy (EDS) and Fourier transform infrared spectroscopy (FTIR). The corrosion properties were tested using the potentiodynamic polarization method in 0.15 M NaCl. The results show that the PEO coatings had significantly higher corrosion resistance than the AZ31 alloy. The PEO coating prepared in the presence of 5 mg/l humic acid (10 min deposition) appeared to have slightly better corrosion resistance than the PEO coating prepared in the absence of humic acid.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
—
OECD FORD obor
20506 - Coating and films
Návaznosti výsledku
Projekt
—
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2024
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
32ND INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, METAL 2023
ISBN
978-80-88365-06-8
ISSN
2694-9296
e-ISSN
—
Počet stran výsledku
5
Strana od-do
512-516
Název nakladatele
Tanger Ltd
Místo vydání
Ostrava
Místo konání akce
Brno
Datum konání akce
17. 5. 2023
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku