Microstructural changes during deformation of AISI 300 grade austenitic stainless steels: Impact of chemical heterogeneity
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26620%2F16%3APU125317" target="_blank" >RIV/00216305:26620/16:PU125317 - isvavai.cz</a>
Výsledek na webu
<a href="https://www.sciencedirect.com/science/article/pii/S2452321616302992" target="_blank" >https://www.sciencedirect.com/science/article/pii/S2452321616302992</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.prostr.2016.06.288" target="_blank" >10.1016/j.prostr.2016.06.288</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Microstructural changes during deformation of AISI 300 grade austenitic stainless steels: Impact of chemical heterogeneity
Popis výsledku v původním jazyce
The present work points out the importance of chemical heterogeneity on the destabilization of austenitic structure and the formation of deformation induced martensite (DIM) in AISI 300 grade austenitic stainless steels (ASSs) of different level of austenite stability (316L, 304, 301LN). Color etching reveals that the structure of wrought Cr-Ni type steels is never fully chemically homogeneous. Confrontation of distribution and morphology of DIM formed in the volume of material after static and cyclic straining under well controlled different conditions with the characteristic local variations in chemical composition of diverse wrought semi-product forms (plates, sheets, bars) proved prominent and very important role of chemical banding in the destabilization of originally fully austenitic structure. This fact should be considered especially when interpreting the results of hydrogen embrittlement tensile testing of Cr-Ni ASSs with lowered Ni content. An impact of chemical heterogeneity on microstructural changes during production of UFG structure of 301LN and its cyclic straining is highlighted.
Název v anglickém jazyce
Microstructural changes during deformation of AISI 300 grade austenitic stainless steels: Impact of chemical heterogeneity
Popis výsledku anglicky
The present work points out the importance of chemical heterogeneity on the destabilization of austenitic structure and the formation of deformation induced martensite (DIM) in AISI 300 grade austenitic stainless steels (ASSs) of different level of austenite stability (316L, 304, 301LN). Color etching reveals that the structure of wrought Cr-Ni type steels is never fully chemically homogeneous. Confrontation of distribution and morphology of DIM formed in the volume of material after static and cyclic straining under well controlled different conditions with the characteristic local variations in chemical composition of diverse wrought semi-product forms (plates, sheets, bars) proved prominent and very important role of chemical banding in the destabilization of originally fully austenitic structure. This fact should be considered especially when interpreting the results of hydrogen embrittlement tensile testing of Cr-Ni ASSs with lowered Ni content. An impact of chemical heterogeneity on microstructural changes during production of UFG structure of 301LN and its cyclic straining is highlighted.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20301 - Mechanical engineering
Návaznosti výsledku
Projekt
<a href="/cs/project/LM2011020" target="_blank" >LM2011020: CEITEC ? open access</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2016
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Procedia Structural Integrity
ISSN
2452-3216
e-ISSN
—
Svazek periodika
2
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
IT - Italská republika
Počet stran výsledku
8
Strana od-do
2299-2306
Kód UT WoS článku
000387976802045
EID výsledku v databázi Scopus
—