Thin high-strength zirconia tapes with extreme flexibility
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26620%2F21%3APU142118" target="_blank" >RIV/00216305:26620/21:PU142118 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/68081723:_____/21:00543756
Výsledek na webu
<a href="https://www.tandfonline.com/doi/full/10.1080/21870764.2021.1930744" target="_blank" >https://www.tandfonline.com/doi/full/10.1080/21870764.2021.1930744</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1080/21870764.2021.1930744" target="_blank" >10.1080/21870764.2021.1930744</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Thin high-strength zirconia tapes with extreme flexibility
Popis výsledku v původním jazyce
The yttria stabilized zirconia ceramics (Y-TZP) are known for their high fracture toughness and high strength. Due to their excellent mechanical properties, the thin zirconia tapes can possess extraordinary behavior - extreme flexibility. In the present work, we introduce an adaptation of gel-tape casting method for the preparation of thin, high-strength zirconia tapes from water-based suspensions. Fine ceramic powder with a particle size of around 100 nm was used. The negative effect of sodium ions on the strength and toughness of sintered ceramic samples was revealed and explained. Ceramic tapes with a thickness of 190 mu m with as-sintered surfaces reached a characteristic biaxial strength of 1805 MPa. The huge elastic deformation of ceramic tapes was demonstrated in a 3- point bend test, and a bending radius of 25 mm for a 75 mu m thick tape was reached.
Název v anglickém jazyce
Thin high-strength zirconia tapes with extreme flexibility
Popis výsledku anglicky
The yttria stabilized zirconia ceramics (Y-TZP) are known for their high fracture toughness and high strength. Due to their excellent mechanical properties, the thin zirconia tapes can possess extraordinary behavior - extreme flexibility. In the present work, we introduce an adaptation of gel-tape casting method for the preparation of thin, high-strength zirconia tapes from water-based suspensions. Fine ceramic powder with a particle size of around 100 nm was used. The negative effect of sodium ions on the strength and toughness of sintered ceramic samples was revealed and explained. Ceramic tapes with a thickness of 190 mu m with as-sintered surfaces reached a characteristic biaxial strength of 1805 MPa. The huge elastic deformation of ceramic tapes was demonstrated in a 3- point bend test, and a bending radius of 25 mm for a 75 mu m thick tape was reached.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20504 - Ceramics
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2021
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Journal of Asian Ceramic Societies
ISSN
2187-0764
e-ISSN
—
Svazek periodika
9
Číslo periodika v rámci svazku
3
Stát vydavatele periodika
JP - Japonsko
Počet stran výsledku
11
Strana od-do
964-974
Kód UT WoS článku
000663653400001
EID výsledku v databázi Scopus
2-s2.0-85108328859