An effect of laser hardening on contact and bending fatigue of a 42CrMo4 steel
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F25797000%3A_____%2F16%3AN0000031" target="_blank" >RIV/25797000:_____/16:N0000031 - isvavai.cz</a>
Výsledek na webu
<a href="http://www.scientific.net/KEM.665.221" target="_blank" >http://www.scientific.net/KEM.665.221</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.4028/www.scientific.net/KEM.665.221" target="_blank" >10.4028/www.scientific.net/KEM.665.221</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
An effect of laser hardening on contact and bending fatigue of a 42CrMo4 steel
Popis výsledku v původním jazyce
The paper deals with an investigation of surface laser hardening characteristics on contact and bending fatigue resistance of a 42CrMo4 steel, being often used for manufacture of gear wheels. The aim of the experimental programme was to simulate the complex service loading of fairly large gears by two separate investigations, namely contact fatigue performed on a special, so called analogon machine and bending fatigue performed on high cycle fatigue resonance machines using three-point-bend (3PB) fairly large specimens. It was shown that after optimising the methodology and parameters of the laser hardening technology, contact fatigue resistance is very good, comparable with very expensive and time consuming thermochemical high-depth surface treatments. Bending endurance limit can be increased. The role of residual stresses resulting from the laser treatment was shown as decisive.
Název v anglickém jazyce
An effect of laser hardening on contact and bending fatigue of a 42CrMo4 steel
Popis výsledku anglicky
The paper deals with an investigation of surface laser hardening characteristics on contact and bending fatigue resistance of a 42CrMo4 steel, being often used for manufacture of gear wheels. The aim of the experimental programme was to simulate the complex service loading of fairly large gears by two separate investigations, namely contact fatigue performed on a special, so called analogon machine and bending fatigue performed on high cycle fatigue resonance machines using three-point-bend (3PB) fairly large specimens. It was shown that after optimising the methodology and parameters of the laser hardening technology, contact fatigue resistance is very good, comparable with very expensive and time consuming thermochemical high-depth surface treatments. Bending endurance limit can be increased. The role of residual stresses resulting from the laser treatment was shown as decisive.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JL - Únava materiálu a lomová mechanika
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/FR-TI3%2F814" target="_blank" >FR-TI3/814: Optimalizace laserového povrchového zpracování strojních součástí pro zvýšení jejich užitných vlastností</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2016
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Key Engineering Materials
ISBN
—
ISSN
10139826
e-ISSN
—
Počet stran výsledku
4
Strana od-do
221-224
Název nakladatele
Trans Tech Publications Ltd
Místo vydání
—
Místo konání akce
Budva
Datum konání akce
21. 9. 2015
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—