Stresses and fatigue of laser welds
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F25797000%3A_____%2F18%3AN0000023" target="_blank" >RIV/25797000:_____/18:N0000023 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/68407700:21340/18:00327176
Výsledek na webu
<a href="https://www.sciencedirect.com/science/article/pii/S2212827118309284" target="_blank" >https://www.sciencedirect.com/science/article/pii/S2212827118309284</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.procir.2018.08.142" target="_blank" >10.1016/j.procir.2018.08.142</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Stresses and fatigue of laser welds
Popis výsledku v původním jazyce
The paper deals with the specific properties of laser welds in fine-grained high-strength steels. The main topic, however, are residual stresses in laser welds, their impact on the mechanical properties and fatigue behaviour of such welds. As documented, fatigue cracks initiate mainly on micropores or other subsurface defects. From X-ray diffraction studies it follows that thermal expansion is primarily responsible for the longitudinal tensile stresses, whereas transverse compressive stresses are caused by phase transformations. The behaviour of transverse stresses also explains why fractures in laser welds occur completely outside the weld metal and the heat-affected zone.
Název v anglickém jazyce
Stresses and fatigue of laser welds
Popis výsledku anglicky
The paper deals with the specific properties of laser welds in fine-grained high-strength steels. The main topic, however, are residual stresses in laser welds, their impact on the mechanical properties and fatigue behaviour of such welds. As documented, fatigue cracks initiate mainly on micropores or other subsurface defects. From X-ray diffraction studies it follows that thermal expansion is primarily responsible for the longitudinal tensile stresses, whereas transverse compressive stresses are caused by phase transformations. The behaviour of transverse stresses also explains why fractures in laser welds occur completely outside the weld metal and the heat-affected zone.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
—
OECD FORD obor
20500 - Materials engineering
Návaznosti výsledku
Projekt
<a href="/cs/project/TH02010664" target="_blank" >TH02010664: Inovativní metody svařování vysokotlakých zařízení s využitím laserových technologií</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2018
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
10th CIRP Conference on Photonic Technologies [LANE 2018]
ISBN
—
ISSN
2212-8271
e-ISSN
—
Počet stran výsledku
4
Strana od-do
481-484
Název nakladatele
Elsevier B.V.
Místo vydání
Amsterdam
Místo konání akce
Furth
Datum konání akce
3. 9. 2018
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—