Microstructure behaviour of AlMgSi alloy processed by ECAP and its thermal stability
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F26316919%3A_____%2F10%3A%230000230" target="_blank" >RIV/26316919:_____/10:#0000230 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Microstructure behaviour of AlMgSi alloy processed by ECAP and its thermal stability
Popis výsledku v původním jazyce
In present study an AlMgSi alloy (AW6082) was an experimental material for deformation experiment carried out severe plastic deformation using ECAP. Aluminium alloy was prepared with three different initial structural states prior ECAP deformation at increased temperature. Substructure and grain refinement of alloy was then investigated by TEM after successive application of different effective strain applied. Hardness and tensile properties were then evaluated with respect to strain level executed. Structure stability and changes in mechanical properties were related to applied strain at two different temperatures of 270 and 350°C. The effect of different increased temperature and hold time at temperature was then monitored with respect to structuralchanges and hardness.
Název v anglickém jazyce
Microstructure behaviour of AlMgSi alloy processed by ECAP and its thermal stability
Popis výsledku anglicky
In present study an AlMgSi alloy (AW6082) was an experimental material for deformation experiment carried out severe plastic deformation using ECAP. Aluminium alloy was prepared with three different initial structural states prior ECAP deformation at increased temperature. Substructure and grain refinement of alloy was then investigated by TEM after successive application of different effective strain applied. Hardness and tensile properties were then evaluated with respect to strain level executed. Structure stability and changes in mechanical properties were related to applied strain at two different temperatures of 270 and 350°C. The effect of different increased temperature and hold time at temperature was then monitored with respect to structuralchanges and hardness.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2010
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Proceedings of 12th International Conference on Aluminium Alloys, 2010
ISBN
978-4-905829-11-9
ISSN
—
e-ISSN
—
Počet stran výsledku
6
Strana od-do
—
Název nakladatele
The Japan Institute of Light Metals,
Místo vydání
Chuo-ku, Tokyo, Japan
Místo konání akce
Yokohama, Japan
Datum konání akce
5. 9. 2010
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—