Optimization of MoNiCr Alloy Production Through Additive Manufacturing
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F26722445%3A_____%2F24%3AN0000039" target="_blank" >RIV/26722445:_____/24:N0000039 - isvavai.cz</a>
Výsledek na webu
<a href="https://www.mdpi.com/1996-1944/18/1/42" target="_blank" >https://www.mdpi.com/1996-1944/18/1/42</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.3390/ma18010042" target="_blank" >10.3390/ma18010042</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Optimization of MoNiCr Alloy Production Through Additive Manufacturing
Popis výsledku v původním jazyce
One of the concepts behind Generation IV reactors is a molten salt coolant system, where the materials for the reactor itself and for the primary and secondary circuit components are subjected to extreme chemical and thermal stresses. Due to the unavailability of these materials, a nickel-molybdenum alloy known as MoNiCr has been developed in the Czech Republic. This paper discusses the manufacturing process for the MoNiCr alloy, covering conventional casting technology, forming, powder atomization, additive manufacturing (AM) using the directed energy deposition (DED-LB) process, and final heat treatment. Special attention was given to the quality of the input powders for additive manufacturing, particularly regarding the optimization of the chemical composition, which significantly influenced the quality of the additively manufactured components. AM enables the realization of complex structural designs that are critical for energy applications, despite the high susceptibility of the MoNiCr alloy to solidification cracking. Through AM, a test body was successfully produced with a maximum defect rate of 0.03% and the following mechanical properties: a yield strength (YS) of 279 MPa, an ultimate tensile strength (UTS) of 602 MPa, and an elongation (El) of 51%.
Název v anglickém jazyce
Optimization of MoNiCr Alloy Production Through Additive Manufacturing
Popis výsledku anglicky
One of the concepts behind Generation IV reactors is a molten salt coolant system, where the materials for the reactor itself and for the primary and secondary circuit components are subjected to extreme chemical and thermal stresses. Due to the unavailability of these materials, a nickel-molybdenum alloy known as MoNiCr has been developed in the Czech Republic. This paper discusses the manufacturing process for the MoNiCr alloy, covering conventional casting technology, forming, powder atomization, additive manufacturing (AM) using the directed energy deposition (DED-LB) process, and final heat treatment. Special attention was given to the quality of the input powders for additive manufacturing, particularly regarding the optimization of the chemical composition, which significantly influenced the quality of the additively manufactured components. AM enables the realization of complex structural designs that are critical for energy applications, despite the high susceptibility of the MoNiCr alloy to solidification cracking. Through AM, a test body was successfully produced with a maximum defect rate of 0.03% and the following mechanical properties: a yield strength (YS) of 279 MPa, an ultimate tensile strength (UTS) of 602 MPa, and an elongation (El) of 51%.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
10403 - Physical chemistry
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2024
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Materials
ISSN
1996-1944
e-ISSN
—
Svazek periodika
18
Číslo periodika v rámci svazku
42
Stát vydavatele periodika
CH - Švýcarská konfederace
Počet stran výsledku
19
Strana od-do
1-19
Kód UT WoS článku
001393628700001
EID výsledku v databázi Scopus
2-s2.0-85214538259