Crack detection and monitoring of their growth in critical parts of steam pipeline by electric potential drop method
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F26722445%3A_____%2F25%3AN0000032" target="_blank" >RIV/26722445:_____/25:N0000032 - isvavai.cz</a>
Výsledek na webu
<a href="https://journalmt.com/artkey/mft-202504-0001_crack-detection-and-monitoring-of-their-growth-in-critical-parts-of-steam-pipeline-by-electric-potential-drop-m.php" target="_blank" >https://journalmt.com/artkey/mft-202504-0001_crack-detection-and-monitoring-of-their-growth-in-critical-parts-of-steam-pipeline-by-electric-potential-drop-m.php</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.21062/mft.2025.046" target="_blank" >10.21062/mft.2025.046</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Crack detection and monitoring of their growth in critical parts of steam pipeline by electric potential drop method
Popis výsledku v původním jazyce
An innovative way of using DCPD (Direct Current Potential Drop) method for off-line and online monitoring of critical parts of energy equipment in operation is presented. There are only a few NDT methods that allow detection and monitoring of defect growth in components at high temperatures and pressures. Monitoring of steam pipes and critical pipeline components in operation has been carried out for several years with different results. a relatively new way of using the DCPD method outside the laboratory is described. The carried-out tests were intended to resemble operational loads as much as possible. Therefore, the tests were performed at a temperature of 20 °C and at an increased temperature of 550 °C. By gradually deepening the groove (slot) simulating the crack type defect in predefined steps, the growth of the defect was simulated up to the full wall thickness of the test sample. The primary evaluation was carried out from the absolute and relative values of measured resistance. The disadvantage of these values is their dependence on the temperature of the monitored area of the test sample and on possibly interfering DC voltages.
Název v anglickém jazyce
Crack detection and monitoring of their growth in critical parts of steam pipeline by electric potential drop method
Popis výsledku anglicky
An innovative way of using DCPD (Direct Current Potential Drop) method for off-line and online monitoring of critical parts of energy equipment in operation is presented. There are only a few NDT methods that allow detection and monitoring of defect growth in components at high temperatures and pressures. Monitoring of steam pipes and critical pipeline components in operation has been carried out for several years with different results. a relatively new way of using the DCPD method outside the laboratory is described. The carried-out tests were intended to resemble operational loads as much as possible. Therefore, the tests were performed at a temperature of 20 °C and at an increased temperature of 550 °C. By gradually deepening the groove (slot) simulating the crack type defect in predefined steps, the growth of the defect was simulated up to the full wall thickness of the test sample. The primary evaluation was carried out from the absolute and relative values of measured resistance. The disadvantage of these values is their dependence on the temperature of the monitored area of the test sample and on possibly interfering DC voltages.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2025
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Manufacturing Technology
ISSN
1213-2489
e-ISSN
2787-9402
Svazek periodika
25
Číslo periodika v rámci svazku
4
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
6
Strana od-do
569-574
Kód UT WoS článku
001605607700014
EID výsledku v databázi Scopus
—