Effect of thermo-oxidative ageing on changes of physical-mechanical parameters of aramid and UHMWPE laminates
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F29372259%3A_____%2F24%3AN0000007" target="_blank" >RIV/29372259:_____/24:N0000007 - isvavai.cz</a>
Výsledek na webu
<a href="https://iopscience.iop.org/article/10.1088/1742-6596/2792/1/012007/pdf" target="_blank" >https://iopscience.iop.org/article/10.1088/1742-6596/2792/1/012007/pdf</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1088/1742-6596/2792/1/012007" target="_blank" >10.1088/1742-6596/2792/1/012007</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Effect of thermo-oxidative ageing on changes of physical-mechanical parameters of aramid and UHMWPE laminates
Popis výsledku v původním jazyce
This work is focused on monitoring of the effect of thermo-oxidative ageing of laminates on their physical-mechanical parameters, such as tensile strength, tensile modulus of elasticity, flexural strength, flexural modulus of elasticity and hardness. Changes of mentioned parameters were observed on two types of laminates based on aramid and two types based on UHMWPE (Ultra High Molecular Weight Polyethylene). The laminates were exposed to the accelerated thermo-oxidative ageing under higher temperature in the presence of atmospheric oxygen. The aim of the work was to find the physical-mechanical parameter with the greatest changes caused by thermo-oxidative ageing. This parameter was consequently chosen for the prediction of laminates lifetime. From the obtained results, it can be seen that aramid laminates show a significantly higher temperature resistance compared to UHWPE-based laminates.
Název v anglickém jazyce
Effect of thermo-oxidative ageing on changes of physical-mechanical parameters of aramid and UHMWPE laminates
Popis výsledku anglicky
This work is focused on monitoring of the effect of thermo-oxidative ageing of laminates on their physical-mechanical parameters, such as tensile strength, tensile modulus of elasticity, flexural strength, flexural modulus of elasticity and hardness. Changes of mentioned parameters were observed on two types of laminates based on aramid and two types based on UHMWPE (Ultra High Molecular Weight Polyethylene). The laminates were exposed to the accelerated thermo-oxidative ageing under higher temperature in the presence of atmospheric oxygen. The aim of the work was to find the physical-mechanical parameter with the greatest changes caused by thermo-oxidative ageing. This parameter was consequently chosen for the prediction of laminates lifetime. From the obtained results, it can be seen that aramid laminates show a significantly higher temperature resistance compared to UHWPE-based laminates.
Klasifikace
Druh
J<sub>SC</sub> - Článek v periodiku v databázi SCOPUS
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2024
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Journal of Physics: Conference Series
ISSN
1742-6588
e-ISSN
—
Svazek periodika
—
Číslo periodika v rámci svazku
2792 012007
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
7
Strana od-do
—
Kód UT WoS článku
—
EID výsledku v databázi Scopus
2-s2.0-85200268120