Pile-Up Correction of Mechanical Characteristics of Individual Phases in Various Steel by Depth Sensing Indentation
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F46747885%3A24210%2F15%3A00002413" target="_blank" >RIV/46747885:24210/15:00002413 - isvavai.cz</a>
Výsledek na webu
<a href="http://www.scientific.net/KEM.662.7" target="_blank" >http://www.scientific.net/KEM.662.7</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.4028/www.scientific.net/KEM.662.7" target="_blank" >10.4028/www.scientific.net/KEM.662.7</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Pile-Up Correction of Mechanical Characteristics of Individual Phases in Various Steel by Depth Sensing Indentation
Popis výsledku v původním jazyce
The Oliver?Pharr method has extensively been adopted for measuring hardness and elastic modulus by indentation techniques. However, the method assumes that the contact periphery sinks in, which limits the applicability to the materials pile-up [1]. Thisstudy proposes an improved methodology to calculate the real mechanical characteristics of individual phases in various steels with significant pile-up. Pile-up correction of mechanical characteristics is based on ratio of pile-up height and contact depth. Pile-up height was measured by atomic force microscopy (AFM). The effect of grain boundaries on the shape and size of the pile-up lobes was also discussed.
Název v anglickém jazyce
Pile-Up Correction of Mechanical Characteristics of Individual Phases in Various Steel by Depth Sensing Indentation
Popis výsledku anglicky
The Oliver?Pharr method has extensively been adopted for measuring hardness and elastic modulus by indentation techniques. However, the method assumes that the contact periphery sinks in, which limits the applicability to the materials pile-up [1]. Thisstudy proposes an improved methodology to calculate the real mechanical characteristics of individual phases in various steels with significant pile-up. Pile-up correction of mechanical characteristics is based on ratio of pile-up height and contact depth. Pile-up height was measured by atomic force microscopy (AFM). The effect of grain boundaries on the shape and size of the pile-up lobes was also discussed.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2015
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Key Engineering Materials vol.662: Mechanical Properties of Materials from Nano to Micro/Meso-Scale
ISBN
978-3-03835-555-7
ISSN
1013-9826
e-ISSN
—
Počet stran výsledku
4
Strana od-do
7-10
Název nakladatele
Trans Tech Publications Inc.
Místo vydání
Churerstrasse 20, CH-8808 Pfaffikon, Switzerland
Místo konání akce
High Tatras, Slovak Republic
Datum konání akce
1. 1. 2014
Typ akce podle státní příslušnosti
EUR - Evropská akce
Kód UT WoS článku
—