Strength of the adhesive joints at the car-body parts from the ahss with al-si coating
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F46747885%3A24210%2F17%3A00004702" target="_blank" >RIV/46747885:24210/17:00004702 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.17973/MMSJ.2017_11_201750" target="_blank" >http://dx.doi.org/10.17973/MMSJ.2017_11_201750</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.17973/MMSJ.2017_11_201750" target="_blank" >10.17973/MMSJ.2017_11_201750</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Strength of the adhesive joints at the car-body parts from the ahss with al-si coating
Popis výsledku v původním jazyce
The paper deals with the monitoring the utility properties of the Al-Si coating which is applied by means of the hot dip coating on the ultra-high strength sheet 22MnB5 (martensite steel alloyed by boron). These sheets are used at the car-body design as the safety elements (bumpers, reinforcement posts). Individual parts are jointed also by the adhesive bonding methods. Evaluation of the material surface protection layers is carried out in dependence on the time of material heating in the furnace during thermal treatment and subsequent influence of this layer on the adhesive joint strength and failure pattern. To compare adhesive joint strength is used epoxy adhesive from two producers. Results provide information about behavior of the ultra-high strength sheets adhesive joints strength properties as a criterion for suitability to apply coatings AlSi in the series production of cars.
Název v anglickém jazyce
Strength of the adhesive joints at the car-body parts from the ahss with al-si coating
Popis výsledku anglicky
The paper deals with the monitoring the utility properties of the Al-Si coating which is applied by means of the hot dip coating on the ultra-high strength sheet 22MnB5 (martensite steel alloyed by boron). These sheets are used at the car-body design as the safety elements (bumpers, reinforcement posts). Individual parts are jointed also by the adhesive bonding methods. Evaluation of the material surface protection layers is carried out in dependence on the time of material heating in the furnace during thermal treatment and subsequent influence of this layer on the adhesive joint strength and failure pattern. To compare adhesive joint strength is used epoxy adhesive from two producers. Results provide information about behavior of the ultra-high strength sheets adhesive joints strength properties as a criterion for suitability to apply coatings AlSi in the series production of cars.
Klasifikace
Druh
J<sub>SC</sub> - Článek v periodiku v databázi SCOPUS
CEP obor
—
OECD FORD obor
20506 - Coating and films
Návaznosti výsledku
Projekt
—
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2017
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
MM Science Journal
ISSN
18031269
e-ISSN
—
Svazek periodika
Vol. 2017
Číslo periodika v rámci svazku
November
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
4
Strana od-do
1901-1904
Kód UT WoS článku
—
EID výsledku v databázi Scopus
2-s2.0-85034646536