Method of Production of High-Strength hollow Bodies from Multiphase Martensitic Steels
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F49777513%3A23210%2F14%3A43922199" target="_blank" >RIV/49777513:23210/14:43922199 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Method of Production of High-Strength hollow Bodies from Multiphase Martensitic Steels
Popis výsledku v původním jazyce
The method of production of high-strength hollow bodies from multiphase martensitic steels includes a heating process, a forming process and a cooling process. The device for heating is used to heat the hollow steel stock to the austenitic temperature ofthe material from which the stock is made. Then, the stock is converted by means of deformation in the forming device into a hollow body having the final shape. Immediately thereafter, the hollow body having the final shape is cooled in the cooling device in such a way that the material with the original austenite microstructure refined by deformation introduced during the forming process is cooled down to a temperature, at which incomplete transformation of austenite to martensite takes place. Immediately thereafter the retained austenite stabilization is performed in the annealing device by diffusion-based carbon partitioning within the material from which the hollow body is made. Once the stabilization is finished, the hollow body i
Název v anglickém jazyce
Method of Production of High-Strength hollow Bodies from Multiphase Martensitic Steels
Popis výsledku anglicky
The method of production of high-strength hollow bodies from multiphase martensitic steels includes a heating process, a forming process and a cooling process. The device for heating is used to heat the hollow steel stock to the austenitic temperature ofthe material from which the stock is made. Then, the stock is converted by means of deformation in the forming device into a hollow body having the final shape. Immediately thereafter, the hollow body having the final shape is cooled in the cooling device in such a way that the material with the original austenite microstructure refined by deformation introduced during the forming process is cooled down to a temperature, at which incomplete transformation of austenite to martensite takes place. Immediately thereafter the retained austenite stabilization is performed in the annealing device by diffusion-based carbon partitioning within the material from which the hollow body is made. Once the stabilization is finished, the hollow body i
Klasifikace
Druh
P - Patent
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2014
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Číslo patentu nebo vzoru
US8852367B2
Vydavatel
US001 -
Název vydavatele
United States Patent and Trademark Office (USPTO)
Místo vydání
Alexandria
Stát vydání
US - Spojené státy americké
Datum přijetí
7. 10. 2014
Název vlastníka
Západočeská univerzita v Plzni
Způsob využití
A - Výsledek využívá pouze poskytovatel
Druh možnosti využití
A - K využití výsledku jiným subjektem je vždy nutné nabytí licence