Influence of deep cryogenic processing on carbide grain size in sintered carbide WC-Co
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F49777513%3A23210%2F21%3A43962144" target="_blank" >RIV/49777513:23210/21:43962144 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/49777513:23640/21:43962144
Výsledek na webu
<a href="https://www.journalmt.com/pdfs/mft/2021/01/04.pdf" target="_blank" >https://www.journalmt.com/pdfs/mft/2021/01/04.pdf</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.21062/mft.2021.004" target="_blank" >10.21062/mft.2021.004</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Influence of deep cryogenic processing on carbide grain size in sintered carbide WC-Co
Popis výsledku v původním jazyce
The paper deals with the change in carbide grain size of sintered WC-Co carbide after cryogenic pro-cessing. Because this structural parameter has a significant effect on mechanical properties. Some sources indicate that due to cryogenic processing takes place to reduce the size of carbide grains and other sources indicate that takes place to increase the size of carbide grains. Measurement of the grain size can be performed using several methods. In this paper, a comparative method according to the ASTM B 390 standard was used. Further, the linear intersection method according to the ČSN ISO 4499-2 standard was used. The last one for measuring the grain size the image analysis software NIS – Elements AR v. 4.40 was used. Also, the size of the WC crystallites by XRD was measured. Crystallites are coherent diffraction domains in X-ray diffraction. The results show that due to cryo-genic processing, the carbide grain increases but the size of the WC crystallites was decreasing.
Název v anglickém jazyce
Influence of deep cryogenic processing on carbide grain size in sintered carbide WC-Co
Popis výsledku anglicky
The paper deals with the change in carbide grain size of sintered WC-Co carbide after cryogenic pro-cessing. Because this structural parameter has a significant effect on mechanical properties. Some sources indicate that due to cryogenic processing takes place to reduce the size of carbide grains and other sources indicate that takes place to increase the size of carbide grains. Measurement of the grain size can be performed using several methods. In this paper, a comparative method according to the ASTM B 390 standard was used. Further, the linear intersection method according to the ČSN ISO 4499-2 standard was used. The last one for measuring the grain size the image analysis software NIS – Elements AR v. 4.40 was used. Also, the size of the WC crystallites by XRD was measured. Crystallites are coherent diffraction domains in X-ray diffraction. The results show that due to cryo-genic processing, the carbide grain increases but the size of the WC crystallites was decreasing.
Klasifikace
Druh
J<sub>SC</sub> - Článek v periodiku v databázi SCOPUS
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
—
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2021
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Manufacturing Technology
ISSN
1213-2489
e-ISSN
—
Svazek periodika
21
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
7
Strana od-do
117-123