Influence of drying process of liquid contaminants on adhesive bond strength
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60460709%3A41310%2F15%3A67747" target="_blank" >RIV/60460709:41310/15:67747 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Influence of drying process of liquid contaminants on adhesive bond strength
Popis výsledku v původním jazyce
Regarding effects of environment factors on adhesive bonds belongs among key requirements influencing the adhesive bond strength. The aim of experiments was to set an influence of liquid contaminants on changes of the adhesive bond strength and to set whether a degradation process is an irreversible change that means whether degradation adhesives will restore their strength characteristics depending on the time. The adhesive bonds were placed into three liquid contaminants for the time 1, 2 and 3 months. The testing process was performed after removing specimens from the liquid contaminant (marked as 0), then after 24, 72 and 163 h. A considerable fall of the adhesive bond strength has already occurred in the first phase of the testing that means after1 month of the contamination. The rate of the adhesive bond strength fall caused by the degradation process is in the interval 10 till 92 %. This undesirable process can be subsequently suppressed by a drying process of the liquid contam
Název v anglickém jazyce
Influence of drying process of liquid contaminants on adhesive bond strength
Popis výsledku anglicky
Regarding effects of environment factors on adhesive bonds belongs among key requirements influencing the adhesive bond strength. The aim of experiments was to set an influence of liquid contaminants on changes of the adhesive bond strength and to set whether a degradation process is an irreversible change that means whether degradation adhesives will restore their strength characteristics depending on the time. The adhesive bonds were placed into three liquid contaminants for the time 1, 2 and 3 months. The testing process was performed after removing specimens from the liquid contaminant (marked as 0), then after 24, 72 and 163 h. A considerable fall of the adhesive bond strength has already occurred in the first phase of the testing that means after1 month of the contamination. The rate of the adhesive bond strength fall caused by the degradation process is in the interval 10 till 92 %. This undesirable process can be subsequently suppressed by a drying process of the liquid contam
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JR - Ostatní strojírenství
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2015
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Manufacturing Technology
ISSN
1213-2489
e-ISSN
—
Svazek periodika
15
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
5
Strana od-do
70-74