Effect of saline environment on mechanical properties of structural adhesive bonds
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60460709%3A41310%2F16%3A71433" target="_blank" >RIV/60460709:41310/16:71433 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.11118/actaun201664051609" target="_blank" >http://dx.doi.org/10.11118/actaun201664051609</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.11118/actaun201664051609" target="_blank" >10.11118/actaun201664051609</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Effect of saline environment on mechanical properties of structural adhesive bonds
Popis výsledku v původním jazyce
This study brings new pieces of knowledge about a utilization of an inorganic filler in an area of steel adhesive bonds exposed to a degradation environment. The filler in the form of glass beads with a fraction size 90 ± 20 µm was used within the research. The aim of the research was to evaluate an influence of the degradation environment on a strength of structural two-component epoxy adhesives and a composite material. A preparation of adhesive bonds and a process of testing of the adhesive bonds were in accordance with the modified standard ČSN EN 1465. The degradation environment in a form of 5 % saline solution was used within this experiment. Adhesive bonded testing samples were subjected to a cyclic loading of the saline solution. The adhesive bonds with the filler reached up to 16 % higher adhesive bond strength than the unfilled adhesive bonds. The bonds adhesive bonded with the tested composite adhesive better resisted to the degradation process of ca. 9 %. The cyclic exposure, i.e. dippin
Název v anglickém jazyce
Effect of saline environment on mechanical properties of structural adhesive bonds
Popis výsledku anglicky
This study brings new pieces of knowledge about a utilization of an inorganic filler in an area of steel adhesive bonds exposed to a degradation environment. The filler in the form of glass beads with a fraction size 90 ± 20 µm was used within the research. The aim of the research was to evaluate an influence of the degradation environment on a strength of structural two-component epoxy adhesives and a composite material. A preparation of adhesive bonds and a process of testing of the adhesive bonds were in accordance with the modified standard ČSN EN 1465. The degradation environment in a form of 5 % saline solution was used within this experiment. Adhesive bonded testing samples were subjected to a cyclic loading of the saline solution. The adhesive bonds with the filler reached up to 16 % higher adhesive bond strength than the unfilled adhesive bonds. The bonds adhesive bonded with the tested composite adhesive better resisted to the degradation process of ca. 9 %. The cyclic exposure, i.e. dippin
Klasifikace
Druh
J<sub>SC</sub> - Článek v periodiku v databázi SCOPUS
CEP obor
—
OECD FORD obor
20506 - Coating and films
Návaznosti výsledku
Projekt
—
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2016
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Acta Universitatis Agriculturae et Silviculturae Mendelianae Brunensis
ISSN
1211-8516
e-ISSN
—
Svazek periodika
64
Číslo periodika v rámci svazku
5
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
9
Strana od-do
1609-1617
Kód UT WoS článku
—
EID výsledku v databázi Scopus
2-s2.0-84994518953