3D-moldability of veneers plasticized with water and ammonia
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60460709%3A41320%2F15%3A65397" target="_blank" >RIV/60460709:41320/15:65397 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.15376/biores.10.1.866-876" target="_blank" >http://dx.doi.org/10.15376/biores.10.1.866-876</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.15376/biores.10.1.866-876" target="_blank" >10.15376/biores.10.1.866-876</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
3D-moldability of veneers plasticized with water and ammonia
Popis výsledku v původním jazyce
The 3D-moldability of veneers, as opposed to the moldability of plastic or other materials, is limited because of the characteristics of wood. Veneers can be modified by physical, chemical, or mechanical treatment. We chose water and ammonia-water solutions. After treatment for an established time, the moldability of veneers was examined. The level of concave deflection of a test piece of punch-molded veneer was assessed. Three sets of test pieces were tested by dipping in cold water (20 °C), hot water(95 °C), or a 25% solution of ammonia, for different durations of time. The results showed that the 3D-moldability of veneers increased by 66 to 119% after plasticization by a 25% solution of ammonia, unlike the unmodified veneers with a moisture contentof 7.65%. The increase in moldability was significantly higher in comparison to the veneers modified by dipping in cold water (20 °C) and hot water (95 °C). Futhermore, the relationship between the moisture content of the veneers after t
Název v anglickém jazyce
3D-moldability of veneers plasticized with water and ammonia
Popis výsledku anglicky
The 3D-moldability of veneers, as opposed to the moldability of plastic or other materials, is limited because of the characteristics of wood. Veneers can be modified by physical, chemical, or mechanical treatment. We chose water and ammonia-water solutions. After treatment for an established time, the moldability of veneers was examined. The level of concave deflection of a test piece of punch-molded veneer was assessed. Three sets of test pieces were tested by dipping in cold water (20 °C), hot water(95 °C), or a 25% solution of ammonia, for different durations of time. The results showed that the 3D-moldability of veneers increased by 66 to 119% after plasticization by a 25% solution of ammonia, unlike the unmodified veneers with a moisture contentof 7.65%. The increase in moldability was significantly higher in comparison to the veneers modified by dipping in cold water (20 °C) and hot water (95 °C). Futhermore, the relationship between the moisture content of the veneers after t
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JI - Kompositní materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2015
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
BioResources
ISSN
1930-2126
e-ISSN
—
Svazek periodika
10
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
11
Strana od-do
866-876
Kód UT WoS článku
000351941000071
EID výsledku v databázi Scopus
—