Shear Bond Strength of Two-Layered Hardwood Strips Bonded with Polyvinyl Acetate and Polyurethane Adhesives
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60460709%3A41320%2F17%3A74830" target="_blank" >RIV/60460709:41320/17:74830 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.15376/biores.12.1.495-513" target="_blank" >http://dx.doi.org/10.15376/biores.12.1.495-513</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.15376/biores.12.1.495-513" target="_blank" >10.15376/biores.12.1.495-513</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Shear Bond Strength of Two-Layered Hardwood Strips Bonded with Polyvinyl Acetate and Polyurethane Adhesives
Popis výsledku v původním jazyce
This article deals with the effects of various parameters on the shear bond strength (SBS) of glued wood. A four-factor analysis showed that the combination of only non-densified wood pieces achieves higher shear bond strength values than densified ones. In this case, only the piece combination was a significant factor. The other factors (glue type, wood species, and number of loading cycles) had no significant effect. Although the differences were not large, a higher SBS was achieved in beech wood glued with polyvinyl acetate (PVAc) glue. Glued wood consisting of the combination of densified and non-densified pieces had slightly lower SBS values. In this case, all the factors were statistically significant. Beech wood had a more significant impact on the SBS than aspen wood. The effect of the type of glue showed an opposite trend than that in the previous variant, i.e., a higher SBS was achieved with polyurethane (PUR) glue. Wood subjected to cyclic loading had slightly higher SBS values than non-cy
Název v anglickém jazyce
Shear Bond Strength of Two-Layered Hardwood Strips Bonded with Polyvinyl Acetate and Polyurethane Adhesives
Popis výsledku anglicky
This article deals with the effects of various parameters on the shear bond strength (SBS) of glued wood. A four-factor analysis showed that the combination of only non-densified wood pieces achieves higher shear bond strength values than densified ones. In this case, only the piece combination was a significant factor. The other factors (glue type, wood species, and number of loading cycles) had no significant effect. Although the differences were not large, a higher SBS was achieved in beech wood glued with polyvinyl acetate (PVAc) glue. Glued wood consisting of the combination of densified and non-densified pieces had slightly lower SBS values. In this case, all the factors were statistically significant. Beech wood had a more significant impact on the SBS than aspen wood. The effect of the type of glue showed an opposite trend than that in the previous variant, i.e., a higher SBS was achieved with polyurethane (PUR) glue. Wood subjected to cyclic loading had slightly higher SBS values than non-cy
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20502 - Paper and wood
Návaznosti výsledku
Projekt
<a href="/cs/project/QJ1520042" target="_blank" >QJ1520042: Stanovování množství zbytkové dendromasy na konkrétní pracoviště - těžební prvek v porostní skupině.</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2017
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
BioResources
ISSN
1930-2126
e-ISSN
—
Svazek periodika
12
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
19
Strana od-do
495-513
Kód UT WoS článku
000397065200036