Identifying the Characteristics of Laminated Wood Based on the Values of Deflection Measured during its Bending
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60460709%3A41320%2F17%3A74832" target="_blank" >RIV/60460709:41320/17:74832 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.15376/biores.12.2.2592-2608" target="_blank" >http://dx.doi.org/10.15376/biores.12.2.2592-2608</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.15376/biores.12.2.2592-2608" target="_blank" >10.15376/biores.12.2.2592-2608</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Identifying the Characteristics of Laminated Wood Based on the Values of Deflection Measured during its Bending
Popis výsledku v původním jazyce
This article is aimed at verifying the influence of selected factors (wood species, lamella combination, type of adhesive, number of loading cycles) on the deflection at the proportionality limit Y-E, deflection at the point of rupture Y-MOR, and the ratio between the deflection at the proportionality limit and the deflection at the point of rupture Y-E : Y-MOR. All of the monitored characteristics were evaluated on test specimens made from lamellas of beechwood (Fagus syivatica L.) and aspen wood (Populus tremula L.). The laminated wood consisted of a combination of lamellas that were non-densified and densified to 10% and 20% of their original thickness. Two types of adhesives were used for the research: polyvinyl acetate (PVA) glue and polyurethane (PUR) glue. The results create a database of information that can be used in developing materials with specified properties for its intended use.
Název v anglickém jazyce
Identifying the Characteristics of Laminated Wood Based on the Values of Deflection Measured during its Bending
Popis výsledku anglicky
This article is aimed at verifying the influence of selected factors (wood species, lamella combination, type of adhesive, number of loading cycles) on the deflection at the proportionality limit Y-E, deflection at the point of rupture Y-MOR, and the ratio between the deflection at the proportionality limit and the deflection at the point of rupture Y-E : Y-MOR. All of the monitored characteristics were evaluated on test specimens made from lamellas of beechwood (Fagus syivatica L.) and aspen wood (Populus tremula L.). The laminated wood consisted of a combination of lamellas that were non-densified and densified to 10% and 20% of their original thickness. Two types of adhesives were used for the research: polyvinyl acetate (PVA) glue and polyurethane (PUR) glue. The results create a database of information that can be used in developing materials with specified properties for its intended use.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20502 - Paper and wood
Návaznosti výsledku
Projekt
—
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2017
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
BioResources
ISSN
1930-2126
e-ISSN
—
Svazek periodika
12
Číslo periodika v rámci svazku
2
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
17
Strana od-do
2592-2608
Kód UT WoS článku
000402883700026