Popis výsledku v původním jazyce
Analyses of Art Noveau mosaics from the church of St. Simon and Juda in Dolín near Slaný and from Holovousy, both probably made by the workshop of Viktor Foerster, have shown that the author probably used the glass type Na2O-PbO-SiO2 and that he used thesame glass also for restoration of The Last Judgment mosaic at the Prague Castle in 1890-1910. Despite the fact that lead glasses are more durable than potassium glasses, the material investigations identified corrosion processes on the surface of the glass pieces (tesserae), which depended on their composition. Apart from the analyzed mosaic Na2O-PbO-SiO2 glasses, we also used ancient sodium glasses (Na2O-CaO-SiO2) and potassium glasses (K2O-CaO-SiO2) from archeological finds in Opava to demonstrate different chemical durability of those glasses. We also paid attention to fixation binders used in Art Noveau mosaics. Inappropriate use of gypsum-containing binders is a serious reason of disintegration of the mosaics. Gypsum and gypsum-l
Název v anglickém jazyce
Signs of Degradation of Czech Art Nouveau Mosaic Glass
Popis výsledku anglicky
Analyses of Art Noveau mosaics from the church of St. Simon and Juda in Dolín near Slaný and from Holovousy, both probably made by the workshop of Viktor Foerster, have shown that the author probably used the glass type Na2O-PbO-SiO2 and that he used thesame glass also for restoration of The Last Judgment mosaic at the Prague Castle in 1890-1910. Despite the fact that lead glasses are more durable than potassium glasses, the material investigations identified corrosion processes on the surface of the glass pieces (tesserae), which depended on their composition. Apart from the analyzed mosaic Na2O-PbO-SiO2 glasses, we also used ancient sodium glasses (Na2O-CaO-SiO2) and potassium glasses (K2O-CaO-SiO2) from archeological finds in Opava to demonstrate different chemical durability of those glasses. We also paid attention to fixation binders used in Art Noveau mosaics. Inappropriate use of gypsum-containing binders is a serious reason of disintegration of the mosaics. Gypsum and gypsum-l
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
AL - Umění, architektura, kulturní dědictví
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GAP405%2F12%2F1411" target="_blank" >GAP405/12/1411: Renesanční sklo a počátky barokního sklářství v archeologických nálezech regionu středního Podunají</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2012
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
ACTA ARTIS ACADEMICA 2012, Znalost a praxe ve výtvarném umění
ISBN
978-80-87108-33-8
ISSN
—
e-ISSN
—
Počet stran výsledku
8
Strana od-do
236-243
Název nakladatele
Akademie výtvarných umění v Praze
Místo vydání
Praha
Místo konání akce
Praha
Datum konání akce
21. 11. 2012
Typ akce podle státní příslušnosti
CST - Celostátní akce
Kód UT WoS článku
—