Recovery of rubidium and potassium alums from lithium-bearing minerals
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60461373%3A22310%2F12%3A43894463" target="_blank" >RIV/60461373:22310/12:43894463 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.hydromet.2012.02.010" target="_blank" >http://dx.doi.org/10.1016/j.hydromet.2012.02.010</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.hydromet.2012.02.010" target="_blank" >10.1016/j.hydromet.2012.02.010</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Recovery of rubidium and potassium alums from lithium-bearing minerals
Popis výsledku v původním jazyce
Rubidium was recovered from lithium-contg. soln. from processing zinnwaldite, (KAl(Fe,Li)(Si3Al)O10F2), conc. after Li2CO3 crystn. as a mixt. of rubidium and potassium alums (RbAl(SO4)2.12H2O and KAl(SO4)2.12H2O). The course of individual reactions aiming at rubidium alum sepn. from carbonated solns. contg. potassium as a main contaminant was studied on synthetic solns. Before the alum pptn., the original carbonated soln. was converted to sulfate soln. Rubidium recovery efficiency at least 95% was achieved if the amt. of the pptn. agent (Al2(SO4)3) ranged between 3.5 and 4.0 multiples of stoichiometric amt. related to rubidium concn. in the processed soln. Under such conditions, ppts. obtained contain between 4.10 and 3.62% Rb and from 6.02 to 6.25% Kand consist of on av. 24% rubidium alum and 75% potassium alum.
Název v anglickém jazyce
Recovery of rubidium and potassium alums from lithium-bearing minerals
Popis výsledku anglicky
Rubidium was recovered from lithium-contg. soln. from processing zinnwaldite, (KAl(Fe,Li)(Si3Al)O10F2), conc. after Li2CO3 crystn. as a mixt. of rubidium and potassium alums (RbAl(SO4)2.12H2O and KAl(SO4)2.12H2O). The course of individual reactions aiming at rubidium alum sepn. from carbonated solns. contg. potassium as a main contaminant was studied on synthetic solns. Before the alum pptn., the original carbonated soln. was converted to sulfate soln. Rubidium recovery efficiency at least 95% was achieved if the amt. of the pptn. agent (Al2(SO4)3) ranged between 3.5 and 4.0 multiples of stoichiometric amt. related to rubidium concn. in the processed soln. Under such conditions, ppts. obtained contain between 4.10 and 3.62% Rb and from 6.02 to 6.25% Kand consist of on av. 24% rubidium alum and 75% potassium alum.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GA104%2F07%2F0499" target="_blank" >GA104/07/0499: Výzkum procesů pro separaci sloučenin Li, Rb a Cs</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>Z - Vyzkumny zamer (s odkazem do CEZ)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2012
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Hydrometallurgy
ISSN
0304-386X
e-ISSN
—
Svazek periodika
119
Číslo periodika v rámci svazku
23.2.2012
Stát vydavatele periodika
NL - Nizozemsko
Počet stran výsledku
3
Strana od-do
73-76
Kód UT WoS článku
000304518800010
EID výsledku v databázi Scopus
—