Temperature dependence of Young's modulus of silica refractories
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60461373%3A22310%2F15%3A43898242" target="_blank" >RIV/60461373:22310/15:43898242 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/67985891:_____/15:00472845
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Temperature dependence of Young's modulus of silica refractories
Popis výsledku v původním jazyce
The temperature dependence of Young's modulus of silica refractories exhibiting pore volume fractions in the range 18.6-20.9% is investigated via impulse excitation up to 800-1000 1C and four-point bending up to 500 1C. This temperature dependence exhibits a broad valley approximately below 200 1C, where Young's modulus values decrease to 55-62% of their room temperature magnitude. Upon further heating, Young's modulus increases steeply within a few degrees around 230 1C, followed by an S-shaped increase to maximum values corresponding to 174-282% of the room temperature values. Cooling branches are different from heating branches and do not form closed loops, indicating damage accumulation. Dilatation measurements, polarization microscopy, micromechanical calculations and X-ray phase analysis are used to underpin the conclusion that the observed elastic effects are not caused by phase transitions alone, but are combined effects of phase transitions and microcrack opening and partial c
Název v anglickém jazyce
Temperature dependence of Young's modulus of silica refractories
Popis výsledku anglicky
The temperature dependence of Young's modulus of silica refractories exhibiting pore volume fractions in the range 18.6-20.9% is investigated via impulse excitation up to 800-1000 1C and four-point bending up to 500 1C. This temperature dependence exhibits a broad valley approximately below 200 1C, where Young's modulus values decrease to 55-62% of their room temperature magnitude. Upon further heating, Young's modulus increases steeply within a few degrees around 230 1C, followed by an S-shaped increase to maximum values corresponding to 174-282% of the room temperature values. Cooling branches are different from heating branches and do not form closed loops, indicating damage accumulation. Dilatation measurements, polarization microscopy, micromechanical calculations and X-ray phase analysis are used to underpin the conclusion that the observed elastic effects are not caused by phase transitions alone, but are combined effects of phase transitions and microcrack opening and partial c
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JH - Keramika, žáruvzdorné materiály a skla
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GAP108%2F12%2F1170" target="_blank" >GAP108/12/1170: Porézní keramika s řízenou elasticitou a tepelnou vodivostí</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2015
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Ceramics International
ISSN
0272-8842
e-ISSN
—
Svazek periodika
41
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
BE - Belgické království
Počet stran výsledku
10
Strana od-do
1129-1138