Transparent MgAl2O4 spinel ceramics prepared via sinter-forging
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60461373%3A22310%2F21%3A43923173" target="_blank" >RIV/60461373:22310/21:43923173 - isvavai.cz</a>
Výsledek na webu
<a href="https://doi.org/10.1016/j.jeurceramsoc.2021.02.017" target="_blank" >https://doi.org/10.1016/j.jeurceramsoc.2021.02.017</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.jeurceramsoc.2021.02.017" target="_blank" >10.1016/j.jeurceramsoc.2021.02.017</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Transparent MgAl2O4 spinel ceramics prepared via sinter-forging
Popis výsledku v původním jazyce
Sinter-forging is a shaping and densification technique that has fallen into oblivion today. However, the ignorance of this technique is unjustified. It is shown that sinter-forging can be utilized for preparation of transparent magnesium aluminum spinel (MgAl2O4) ceramics in SPS equipment. While the porosity and grain size of the materials prepared via sinter-forging and conventional SPS with the same process schedule is very similar (0.2-1.1 % and 0.33-0.02 micrometers, respectively) the in-line transmittance (at a wavelength of 550 nm) is 45 % for the material prepared via sinter-forging, but only 3 % for the material prepared via conventional SPS. The reason for this surprisingly high in-line transmittance at relatively high porosity is evidently the pore size, which is much smaller with sinter-forging than with conventional SPS.
Název v anglickém jazyce
Transparent MgAl2O4 spinel ceramics prepared via sinter-forging
Popis výsledku anglicky
Sinter-forging is a shaping and densification technique that has fallen into oblivion today. However, the ignorance of this technique is unjustified. It is shown that sinter-forging can be utilized for preparation of transparent magnesium aluminum spinel (MgAl2O4) ceramics in SPS equipment. While the porosity and grain size of the materials prepared via sinter-forging and conventional SPS with the same process schedule is very similar (0.2-1.1 % and 0.33-0.02 micrometers, respectively) the in-line transmittance (at a wavelength of 550 nm) is 45 % for the material prepared via sinter-forging, but only 3 % for the material prepared via conventional SPS. The reason for this surprisingly high in-line transmittance at relatively high porosity is evidently the pore size, which is much smaller with sinter-forging than with conventional SPS.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20504 - Ceramics
Návaznosti výsledku
Projekt
<a href="/cs/project/GA18-17899S" target="_blank" >GA18-17899S: Částečně a plně slinutá keramika - příprava, mikrostruktura, vlastnosti, modelování a teorie slinování</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2021
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Journal of the European Ceramic Society
ISSN
0955-2219
e-ISSN
—
Svazek periodika
41
Číslo periodika v rámci svazku
7
Stát vydavatele periodika
BE - Belgické království
Počet stran výsledku
6
Strana od-do
4313-4318
Kód UT WoS článku
000632730900001
EID výsledku v databázi Scopus
—