Direct measurement of negative Poisson ratios of auxetic materials via the impulse excitation technique (IET)
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60461373%3A22310%2F24%3A43928644" target="_blank" >RIV/60461373:22310/24:43928644 - isvavai.cz</a>
Výsledek na webu
<a href="https://www.sciencedirect.com/science/article/pii/S0955221923008889?via%3Dihub" target="_blank" >https://www.sciencedirect.com/science/article/pii/S0955221923008889?via%3Dihub</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.jeurceramsoc.2023.10.076" target="_blank" >10.1016/j.jeurceramsoc.2023.10.076</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Direct measurement of negative Poisson ratios of auxetic materials via the impulse excitation technique (IET)
Popis výsledku v původním jazyce
The direct measurement of Poisson ratios via the impulse excitation technique (IET) is based on determining the frequency ratio between the resonant frequencies of flexural and torsional vibrations of circular discs. However, the direct measurement of negative Poisson ratios, which occur in auxetic materials, has been impeded until now by the absence of numerical values of Martinček's solution for frequency ratios smaller than 1.35, because the relevant ASTM standards have not considered the possibility of negative Poisson ratios so far. Here we provide this missing link by reconsidering Martinček's solution and presenting the necessary values in the forms of graphs and fit relations from which the Poisson ratio, including negative ones (down to −0.273), can be determined from frequency ratios down to 1.1 for a wide range of specimen aspect ratios (down to 4). © 2023 Elsevier Ltd
Název v anglickém jazyce
Direct measurement of negative Poisson ratios of auxetic materials via the impulse excitation technique (IET)
Popis výsledku anglicky
The direct measurement of Poisson ratios via the impulse excitation technique (IET) is based on determining the frequency ratio between the resonant frequencies of flexural and torsional vibrations of circular discs. However, the direct measurement of negative Poisson ratios, which occur in auxetic materials, has been impeded until now by the absence of numerical values of Martinček's solution for frequency ratios smaller than 1.35, because the relevant ASTM standards have not considered the possibility of negative Poisson ratios so far. Here we provide this missing link by reconsidering Martinček's solution and presenting the necessary values in the forms of graphs and fit relations from which the Poisson ratio, including negative ones (down to −0.273), can be determined from frequency ratios down to 1.1 for a wide range of specimen aspect ratios (down to 4). © 2023 Elsevier Ltd
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20504 - Ceramics
Návaznosti výsledku
Projekt
<a href="/cs/project/GA22-25562S" target="_blank" >GA22-25562S: Impulzní excitace jako nekonvenční metoda k monitorování fázových přeměn a mikrostrukturních změn během tepelného zatížení materiálů</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2024
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Journal of the European Ceramic Society
ISSN
0955-2219
e-ISSN
1873-619X
Svazek periodika
44
Číslo periodika v rámci svazku
4
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
8
Strana od-do
2338-2345
Kód UT WoS článku
001138906300001
EID výsledku v databázi Scopus
2-s2.0-85177025845